Stresses in proton exchange membranes due to hygro-thermal loading

被引:115
作者
Tang, Yaliang [1 ]
Santare, Michael H.
Karlsson, Anette M.
Cleghorn, Simon
Johnson, William B.
机构
[1] Univ Delaware, Dept Engn Mech, Newark, DE 19716 USA
[2] Gore Fuel Cell Technol, Elkton, MD 21922 USA
来源
JOURNAL OF FUEL CELL SCIENCE AND TECHNOLOGY | 2006年 / 3卷 / 02期
关键词
D O I
10.1115/1.2173666
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Durability of the proton exchange membrane (PEM) is a major technical barrier to the commercial viability of polymer electrolyte membrane fuel cells (PEMFC) for stationary and transportation applications. In. order to reach Department of Energy objectives for automotive PEMFCs, an operating design lifetime of at least 5000 h over a broad temperature range is required. Reaching these lifetimes is an extremely difficult technical challenge. Though good progress has been made in recent years, there are still issues that need to be addressed to assure successful, economically viable, long-term operation of PEM fuel cells. Fuel cell lifetime is currently limited by gradual degradation of both the chemical and hygro-thermomechanical properties of the membranes. Eventually the system fails due to a critical reduction of the voltage or mechanical damage. However, the hygro-thermomechanical loading of the membranes and how this effects the lifetime of the fuel cell is not understood. The long-term objective of the research is to establish a fundamental understanding of the mechanical processes in degradation and how they influence the lifetime of PEMFCs based on perfluorosulfuric acid membrane. In this paper, we discuss the finite element models developed to investigate the in situ stresses in polymer-membranes.
引用
收藏
页码:119 / 124
页数:6
相关论文
共 21 条
[1]  
Benziger J. B., 2003, AICHE ANN M SAN FRAN
[2]   A 3D, multiphase, multicomponent model of the cathode and anode of a PEM fuel cell [J].
Berning, T ;
Djilali, N .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (12) :A1589-A1598
[3]  
BEUSCHER U, 2002, 202 M EL SOC SALT LA
[4]  
BOSSEL UG, 1999, P EUR FUEL CELL FOR, P79
[5]  
*DOE, DEV DEM PLAN PLANN A, P7
[6]   Distributed performance of polymer electrolyte fuel cells under low-humidity conditions [J].
Dong, Q ;
Mench, MM ;
Cleghorn, S ;
Beuscher, U .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (11) :A2114-A2122
[7]  
DONG Q, 2004, 206 M EL SOC HON HI
[8]   WATER AND THERMAL MANAGEMENT IN SOLID-POLYMER-ELECTROLYTE FUEL-CELLS [J].
FULLER, TF ;
NEWMAN, J .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (05) :1218-1225
[9]  
*HIBB KARLSS SOR, 2003, ABAQUS AN US MAN
[10]   A three-dimensional numerical simulation of the transport phenomena in the cathodic side of a PEMFC [J].
Hwang, JJ ;
Chen, CK ;
Savinell, RF ;
Liu, CC ;
Wainright, J .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 2004, 34 (02) :217-224