摘要
The effect of electrolyte temperature on the passivity of solid electrolyte interphase (SET) was investigated in I M LiPF6-ethylene carbonate/diethyl carbonate (50:50 vol.%) electrolyte, using galvanostatic charge-discharge experiment, and ac-impedance spectroscopy combined with Fourier transform infra-red spectroscopy. and high resolution transmission electron microscopy (HRTEM). The galvanostatic charge-discharge curves at 20 degreesC evidenced that the irreversible capacity loss during electrochemical cycling was markedly increased with rising SET formation temperature from 0 to 40 degreesC. This implies that the higher the SET formation temperature. the more were the graphite electrodes exposed to structural damages, From both increase of the relative amount of Li2CO3 to ROCO2Li and decrease of resistance to the lithium transport through the SET layer with increasing SET formation temperature, it is reasonable to claim that, due to the enhanced gas evolution reactions during transformation of ROCO2Li to Li2CO3. the rising SET formation temperature increased the number of defect sites in the SET la er. From the analysis of HRTEM images, no significant structural destruction in bulk graphite layer was observed after charge-discharge cycles. This means that solvated lithium ions were intercalated through the defect sites in the SET, at most, into the surface region of the graphite layer. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2333 / 2339
页数:7
相关论文
共 16 条
[1]   In situ AFM study of interlayer spacing during anion intercalation into HOPG in aqueous electrolyte [J].
Alliata, D ;
Kötz, R ;
Haas, O ;
Siegenthaler, H .
LANGMUIR, 1999, 15 (24) :8483-8489
[2]   Capacity fade mechanisms and side reactions in lithium-ion batteries [J].
Arora, P ;
White, RE ;
Doyle, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (10) :3647-3667
[3]   On the correlation between surface chemistry and performance of graphite negative electrodes for Li ion batteries [J].
Aurbach, D ;
Markovsky, B ;
Weissman, I ;
Levi, E ;
Ein-Eli, Y .
ELECTROCHIMICA ACTA, 1999, 45 (1-2) :67-86
[4]   New insights into the interactions between electrode materials and electrolyte solutions for advanced nonaqueous batteries [J].
Aurbach, D ;
Markovsky, B ;
Levi, MD ;
Levi, E ;
Schechter, A ;
Moshkovich, M ;
Cohen, Y .
JOURNAL OF POWER SOURCES, 1999, 81 :95-111
[5]  
Du Pasquier A, 1998, J ELECTROCHEM SOC, V145, P472
[6]   STM study on graphite/electrolyte interface in lithium-ion batteries: solid electrolyte interface formation in trifluoropropylene carbonate solution [J].
Inaba, M ;
Kawatate, Y ;
Funabiki, A ;
Jeong, SK ;
Abe, T ;
Ogumi, Z .
ELECTROCHIMICA ACTA, 1999, 45 (1-2) :99-105
[7]   Electrochemical scanning tunneling microscopy observation of highly oriented pyrolytic graphite surface reactions in an ethylene carbonate-based electrolyte solution [J].
Inaba, M ;
Siroma, Z ;
Funabiki, A ;
Ogumi, Z ;
Abe, T ;
Mizutani, Y ;
Asano, M .
LANGMUIR, 1996, 12 (06) :1535-1540
[8]  
MOSHOVICH M, 1999, J POWER SOURCES, V81, P95
[9]   THE ELECTROCHEMICAL-BEHAVIOR OF ALKALI AND ALKALINE-EARTH METALS IN NON-AQUEOUS BATTERY SYSTEMS - THE SOLID ELECTROLYTE INTERPHASE MODEL [J].
PELED, E .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (12) :2047-2051
[10]   In-situ spectroelectrochemical analysis of the passivating surface film formed on a graphite electrode during the electrochemical reduction of lithium salts and organic carbonate solvent [J].
Pyun, SI ;
Ryu, YG .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1998, 455 (1-2) :11-17