Osteoinductive ability of human allograft formulations

被引:32
作者
Boyan, Barbara D.
Ranly, Don M.
McMillan, Jacquelyn
Sunwoo, MoonHae
Roche, Karen
Schwartz, Zvi
机构
[1] Georgia Inst Technol, Dept Biomed Engn, Atlanta, GA 30332 USA
[2] Musculoskeletal Transplant Fdn, Edison, NJ USA
[3] Spineol, St Paul, MN USA
[4] Hebrew Univ Jerusalem Hadassah Hosp & Med Sch, Dept Periodont, Jerusalem, Israel
关键词
allograft; bone matrix; humans; hyaluronic acid; mice; nude; muscle;
D O I
10.1902/jop.2006.060019
中图分类号
R78 [口腔科学];
学科分类号
1003 [口腔医学];
摘要
Background: Bone graft materials are needed in periodontics that are osteoinductive, have good handling characteristics, and have physical properties that provide appropriate stiffness for the treatment site. Dermineralized freeze-dried bone allograft (DFDBA), also called demineralized bone matrix (DBM), is osteoinductive but requires a carrier to meet the other clinical objectives, thereby decreasing the DBM content per volume of the bone graft material. The present study determined whether the DBM content of a carrier formulation is an important variable with respect to its effectiveness as an osteoinductive material. Methods: The immunocompromised Nu/Nu mouse-muscle implantation assay of osteoinductivity was used to test human DBM formulated with hyaluronic acid (HY) and cancellous and cortical bone granules from the same donor: DBM alone (I I mg); DBM (11 mg):HY, 55:45, weight/weight (wt/wt); DBM (6.4 mg):HY, 32:68, wt/wt; DBM mixed with cortical and cancellous bone chips 1:4 (DBMC) (11 mg total, of which 2.2 mg was DBM); DBMC (11 mg):HY, 55:45, wt/wt; heat-treated DBM (11 mg); HY alone; and positive-control DBM (11 mg). Osteoinduction was scored using a qualitative scale and by histomorphometry. Results: Results showed that all DBM was osteoinductive and the addition of HY did not change this as long as the amount of DBM used was held constant. The reduction in the absolute amount of DBM resulted in a reduced osteoinduction score, reduced ossicle area, and reduced new bone formation. The addition of HY also caused a decrease in the amount of residual non-vital bone particles, particularly when DBMC was implanted. Results were donor dependent. Conclusion: This study showed the importance of DBM content and donor variability in osteoinductivity of DBM formulations with improved handling and stiffness characteristics.
引用
收藏
页码:1555 / 1563
页数:9
相关论文
共 32 条
[1]
Ascher B, 2004, Ann Chir Plast Esthet, V49, P465, DOI 10.1016/j.anplas.2004.09.001
[2]
BODINE RL, 1970, DENT CLIN N AM, V14, P145
[3]
Comparison of posterolateral lumbar fusion rates of Grafton Putty and OP-1 Putty in an athymic rat model [J].
Bomback, DA ;
Grauer, JN ;
Lugo, R ;
Troiano, N ;
Patel, TC ;
Friedlaender, GE .
SPINE, 2004, 29 (15) :1612-1617
[4]
Boyan BD, 1999, J BIOMED MATER RES, V46, P51, DOI 10.1002/(SICI)1097-4636(199907)46:1<51::AID-JBM6>3.3.CO
[5]
2-9
[6]
Callan D P, 2000, Implant Dent, V9, P36, DOI 10.1097/00008505-200009010-00008
[7]
Quantitative assessment of the tissue response to films of hyaluronan derivatives [J].
Campoccia, D ;
Hunt, JA ;
Doherty, PJ ;
Zhong, SP ;
ORegan, M ;
Benedetti, L ;
Williams, DF .
BIOMATERIALS, 1996, 17 (10) :963-975
[8]
Chen Qing, 2003, Zhongguo Xiu Fu Chong Jian Wai Ke Za Zhi, V17, P5
[9]
Healing response to various forms of human demineralized bone matrix in athymic rat cranial defects [J].
Chesmel, KD ;
Branger, J ;
Wertheim, H ;
Scarborough, N .
JOURNAL OF ORAL AND MAXILLOFACIAL SURGERY, 1998, 56 (07) :857-863
[10]
Fukuda Kanji, 2004, Clin Calcium, V14, P103