Deformation and fracture behavior of two Al-Mg-Si alloys

被引:47
作者
Zhen, L [1 ]
Kang, SB [1 ]
机构
[1] KOREA INST MACHINERY & MAT,CHANG WON 641010,SOUTH KOREA
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1997年 / 28卷 / 07期
关键词
Material Transaction; Aging Time; Slip Plane; Slip Band; Natural Aging;
D O I
10.1007/s11661-997-0211-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Deformation and fracture behavior of two Al-Mg-Si alloys in different aging conditions has been studied by tensile testing, transmission electron microscope (TEM), and scanning electron microscope (SEM) observation. Tensile test results show that the strain hardening exponents (n values) of the two alloys decrease sharply at the early stage of artificial aging and are only 0.045 and 0.06, respectively, in the overaged condition. The sharp decrease of work hardening rate is believed to be one major reason that results in the rapid decrease of elongation to failure at the early stage of artificial aging. In fully aged conditions, dislocations are concentrated in narrow bands during plastic deformation of these alloys, which is responsible for the very low n values of the Al-Mg-Si alloys in peak aged and overaged conditions. The Si particles formed in the interior of grains of the higher Si containing alloy reduce the inhomogeneous deformation behavior. The TEM results show that large precipitates and precipitate-free zones (PFZs) along grain boundaries are formed in peak aged and overaged conditions, and SEM observations demonstrate that the tensile fracture modes of the two alloys in these aging conditions are completely intergranular with many small cusps decorated on facets of the fractured grain boundaries. Thus, the fracture process of both alloys is suggested to be that in which the high local stresses, built up where the slip band impinges on the grain boundaries, nucleate voids at the grain boundary precipitates by decohesion of the particle/PFZ interface, and then coalescence of these voids within the PFZ leads to the final fracture of these alloys.
引用
收藏
页码:1489 / 1497
页数:9
相关论文
共 17 条
[1]   QUANTIFICATION OF THE MG2SI-BETA'' AND BETA' PHASES IN ALMGSI ALLOYS BY TRANSMISSION ELECTRON-MICROSCOPY [J].
ANDERSEN, SJ .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (08) :1931-1937
[2]   TECHNOECONOMIC ISSUES IN THE SELECTION OF AUTO MATERIALS [J].
ARNOLD, SA .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1993, 45 (06) :12-15
[3]   INFLUENCE OF MN ADDITIONS ON DEFORMATION-BEHAVIOR OF AN AL-MG-SI ALLOY [J].
DOWLING, JM ;
MARTIN, JW .
ACTA METALLURGICA, 1976, 24 (12) :1147-1153
[4]   A CALORIMETRIC STUDY OF PRECIPITATION IN COMMERCIAL ALUMINUM ALLOY-6061 [J].
DUTTA, I ;
ALLEN, SM .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1991, 10 (06) :323-326
[5]   EFFECT OF REINFORCEMENT ON THE AGING RESPONSE OF CAST 6061 AL-AL2O3 PARTICULATE COMPOSITES [J].
DUTTA, I ;
ALLEN, SM ;
HAFLEY, JL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11) :2553-2563
[6]  
EDWARDS GA, 1994, P 4 INT C AL ALL ATL, V1, P620
[7]   Effects of cooling rate on solidification process in Al-Mg-Si alloy [J].
Fei, WD ;
Kang, SB .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1995, 14 (24) :1795-1797
[8]  
GUPTA A K, 1994, P 4 INT C AL ALL ICA, V3, P177
[9]   DUCTILE FRACTURE IN INTERIOR OF PRECIPITATE FREE ZONE IN AN AL-6.0-PERCENT ZN-2.6-PERCENT MG ALLOY [J].
KAWABATA, T ;
IZUMI, O .
ACTA METALLURGICA, 1976, 24 (09) :817-825
[10]  
MONDOLFO LE, 1976, ALUMINIUM ALLOYS STR, P788