Polypyrrole thin films formed by admicellar polymerization support the osteogenic differentiation of mesenchymal stem cells

被引:117
作者
Castano, H [1 ]
O'Rear, EA [1 ]
McFetridge, PS [1 ]
Sikavitsas, VI [1 ]
机构
[1] Univ Oklahoma, Bioengn Ctr, Sch Chem Biol & Mat Engn, Norman, OK 73019 USA
关键词
admicellar polymerization; biological applications of polymers; differentiation; mesenchymal stem cells; polypyrrole; osteoblast; thin films;
D O I
10.1002/mabi.200300123
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 [生物化学与分子生物学]; 081704 [应用化学];
摘要
The objective of this study was to evaluate the attachment, proliferation, and differentiation of rat mesenchymal stem cells (MSC) toward the osteoblastic phenotype seeded on polypyrrole (PPy) thin films made by admicellar polymerization. Three different concentrations of pyrrole (Py) monomer (20, 35, and 50 x 10(-3) M) were used with the PPy films deposited on tissue culture polystyrene dishes (TCP). Regular TCP dishes and PPy polymerized on TCP by chemical polymerization without surfactant using 5 x 10-3 M Py, were used as controls. Rat MSC were seeded on these surfaces and cultured for up to 20 d in osteogenic media. Surface topography was characterized by atomic force microscopy, X-ray photoelectron spectroscopy, and static contact angle. Cell attachment, proliferation, alkaline phosphatase (ALP) activity, and calcium content were measured to evaluate the ability of MSC to adhere and differentiate on PPy-coated TCP. Increased monomer concentrations resulted in PPy films of increased thickness and surface roughness. PPy films generated by different monomer concentrations induced drastically different cellular events. A wide spectrum of cell attachment characteristics (from excellent cell attachment to the complete inability to adhere) were obtained by varying the monomer concentration from 20 m to 50 x 10(-3) m. In particular the 20 x 10(-3) m PPy thin films demonstrated superior induction of MSC osteogenicity, which was comparable to standard TCP dishes, unlike PPy films of similar thickness prepared by chemical polymerization without surfactant.
引用
收藏
页码:785 / 794
页数:10
相关论文
共 55 条
[1]
[Anonymous], 1997, 42871997 ISO
[2]
Osteoblast adhesion on biomaterials [J].
Anselme, K .
BIOMATERIALS, 2000, 21 (07) :667-681
[3]
CULTURE OF MAMMALIAN-CELLS ON POLYPYRROLE-COATED ITO AS A BIOCOMPATIBLE ELECTRODE [J].
AOKI, T ;
TANINO, M ;
SANUI, K ;
OGATA, N ;
KUMAKURA, K ;
OKANO, T ;
SAKURAI, Y ;
WATANABE, M .
SYNTHETIC METALS, 1995, 71 (1-3) :2229-2230
[4]
EFFECTS OF ELECTRIC CURRENTS ON BONE IN VIVO [J].
BASSETT, CA ;
PAWLUK, RJ ;
BECKER, RO .
NATURE, 1964, 204 (495) :652-&
[5]
BASSETT CAL, 1974, SCIENCE, V184, P575
[6]
Effect of surface roughness and composition on costochondral chondrocytes is dependent on cell maturation state [J].
Boyan, BD ;
Lincks, J ;
Lohmann, CH ;
Sylvia, VL ;
Cochran, DL ;
Blanchard, CR ;
Dean, DD ;
Schwartz, Z .
JOURNAL OF ORTHOPAEDIC RESEARCH, 1999, 17 (03) :446-457
[7]
DIRECT-CURRENT STIMULATION OF NON-UNION AND CONGENITAL PSEUDARTHROSIS - EXPLORATION OF ITS CLINICAL APPLICATION [J].
BRIGHTON, CT ;
FRIEDENBERG, ZB ;
ZEMSKY, LM ;
POLLIS, PR .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1975, A 57 (03) :368-377
[8]
Signal transduction in electrically stimulated bone cells [J].
Brighton, CT ;
Wang, W ;
Seldes, R ;
Zhang, GH ;
Pollack, SR .
JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 2001, 83A (10) :1514-1523
[9]
BRIGHTON CT, 1977, CLIN ORTHOP RELAT R, V124, P106
[10]
BRIGHTON CT, 1979, ELECTRICAL PROPERTIE, P519