High-temperature mechanical behavior and microstructure of SiC-whisker-reinforced MoSi2 composites

被引:27
作者
Zheng, LY [1 ]
Jin, YP [1 ]
Li, PX [1 ]
机构
[1] SHANGHAI JIAO TONG UNIV,STATE KEY LAB MET MATRIX COMPOSITES,SHANGHAI 200030,PEOPLES R CHINA
关键词
MoSi2; SiC whisker; composite; microstructure; interface;
D O I
10.1016/S0266-3538(96)00169-8
中图分类号
TB33 [复合材料];
学科分类号
摘要
Composites of MoSi2 reinforced with 20 vol% SiC whiskers and samples of the unreinforced matrix material fabricated by hot pressing have been tested in three-point bending at 1200 degrees C. It is found that both materials deform plastically at the test temperature. However, the composites have much higher bending resistance than does the matrix material. The ultimate strengths of the composites and the matrix are about 300 MPa and 170 MPa, respectively, as estimated from the load/deflection curves. Results of SEM and TEM investigations show that there are many pulled-out whiskers wrapped in a thick layer of matrix phase in the tensile stress zone on the fracture surface. The interface of SiCw/MoSi2 is chemically compatible. Stacking faults and a low-melting amorphous phase are also found in the matrix of the composites and are regarded as contributing to the deformation of the materials at high temperatures. Finally, the strengthening mechanisms of SiCw/MoSi2 composites at high temperatures are discussed from the viewpoints of composite strengthening and dislocation strengthening. (C) 1997 Elsevier Science Limited.
引用
收藏
页码:463 / 469
页数:7
相关论文
共 18 条
[1]   STRENGTHENING OF DISCONTINUOUSLY REINFORCED MOSI2 COMPOSITES AT HIGH-TEMPERATURES [J].
AIKIN, RM .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 155 (1-2) :121-133
[2]  
CATER DH, 1989, CERAM ENG SCI P, V10, P1121
[3]   INTRINSIC 2ND-PHASE PARTICLES IN POWDER-PROCESSED MOSI2 [J].
COTTON, JD ;
KIM, YS ;
KAUFMAN, MJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 144 :287-291
[4]  
Gac FD., 1985, J AM CERAM SOC, DOI 10.1111/j.1151-2916.1985.tb10182.x
[5]  
JIN YP, 1994, CHINESE J MAT RES, V8, P183
[6]   TOUGHENING OF MOSI2 WITH A DUCTILE (NIOBIUM) REINFORCEMENT [J].
LU, TC ;
EVANS, AG ;
HECHT, RJ ;
MEHRABIAN, R .
ACTA METALLURGICA ET MATERIALIA, 1991, 39 (08) :1853-1862
[7]   EFFECTS OF CARBON ADDITIONS ON THE HIGH-TEMPERATURE MECHANICAL-PROPERTIES OF MOLYBDENUM DISILICIDE [J].
MALOY, SA ;
LEWANDOWSKI, JJ ;
HEUER, AH ;
PETROVIC, JJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 155 (1-2) :159-163
[8]  
MECHTER PJ, 1989, J MET, V41, P52
[9]   ON THE STRENGTH OF DISCONTINUOUS SILICON-CARBIDE REINFORCED ALUMINUM COMPOSITES [J].
NARDONE, VC ;
PREWO, KM .
SCRIPTA METALLURGICA, 1986, 20 (01) :43-48
[10]  
PETROVIC JJ, 1990, MATER RES SOC SYMP P, V194, P123, DOI 10.1557/PROC-194-123