Hard AlTiN, AlCrNPVD coatings for machining of austenitic stainless steel

被引:209
作者
Endrino, J. L.
Fox-Rabinovich, G. S. [1 ]
Gey, C.
机构
[1] Balzers AG, SBU Tools, FL-9496 Balzers, Liechtenstein
[2] McMaster Univ, Hamilton, ON L8S 4L7, Canada
关键词
hard PVD coatings; machining; stainless steel; cutting tools;
D O I
10.1016/j.surfcoat.2005.10.030
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The austenitic stainless steels in general are considered to be difficult to machine materials. This is mainly due to the high plasticity and tendency to work-harden of the austenitic stainless steel, which usually results in severe cutting conditions. Additionally, austenitic stainless steels have much lower thermal conductivity as compared to structural carbon steels; this inflicts high thermal impact within the chip-tool contact zone, which significantly increase the cutting tool wear rate. The machineability of austenitic stainless steels can be improved due to application of coated cutting tools. Hard PVD coating with low thermal conductivity and improved surface finish should be used in this case. This can result in enhancement of frictional characteristics at the tool/workpiece interface as well as chip evacuation process. In this study the stainless steel plates were machined using cemented carbide finishing end mills with four high aluminum containing PVD coatings namely: AlCrN, AlCrNbN, fine grained (fg) AlTiN and nano-crystalline (nc) AlTiN. Both AlTiN and AlCrN-based coatings have high oxidation resistances due to formation of aluminum oxide surface layers. The influence of surface post-deposition treatment on tool wear intensity was investigated. The coating surface texture before and after post-deposition treatment was analyzed by means of the Abbot-Firestone ratio curves. Minimal wear intensity after length of cut 150 m was achieved for cutting tools with the nc-AlTiN coating. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:6840 / 6845
页数:6
相关论文
共 21 条
[1]   Performance of new AlTiN coatings in dry and high speed cutting [J].
Arndt, M ;
Kacsich, T .
SURFACE & COATINGS TECHNOLOGY, 2003, 163 :674-680
[2]   Improvement of PVD coated inserts cutting performance, through appropriate mechanical treatments of substrate and coating surface [J].
Bouzakis, KD ;
Michailidis, N ;
Hadjiyiannis, S ;
Efstathiou, K ;
Pavlidou, E ;
Erkens, G ;
Rambadt, S ;
Wirth, I .
SURFACE & COATINGS TECHNOLOGY, 2001, 146 :443-450
[3]  
ENDRINO JL, IN PRESS SURF COAT T
[4]   Nano-crystalline filtered arc deposited (FAD) TiAlNPVD coatings for high-speed machining applications [J].
Fox-Rabinovich, GS ;
Weatherly, GC ;
Dodonov, AI ;
Kovalev, AI ;
Shuster, LS ;
Veldhuis, SC ;
Dosbaeva, GK ;
Wainstein, DL ;
Migranov, MS .
SURFACE & COATINGS TECHNOLOGY, 2004, 177 :800-811
[5]   The role of chromium in protective alumina scale formation during the oxidation of ternary TiAlCr alloys in air [J].
Fox-Rabinovich, GS ;
Weatherly, GC ;
Wilkinson, DS ;
Kovalev, AI ;
Wainstein, DL .
INTERMETALLICS, 2004, 12 (02) :165-180
[6]   Nano-crystal alloy and alloy-oxide coatings and their high-temperature corrosion properties [J].
Gao, W ;
Liu, ZY ;
Li, ZW ;
Li, SS ;
Gong, H .
INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2002, 16 (1-2) :128-136
[7]  
HOLMBERG K, 1994, COATING TRIBOLOGY PR, P257
[8]  
IKEDA T, 1991, THIN SOLID FILMS, V195, P99, DOI 10.1016/0040-6090(91)90262-V
[9]  
*ISO, 1996, ISO135652
[10]  
Knotek O., 1992, Surface and Coatings Technology, V54-55, P476, DOI 10.1016/S0257-8972(07)80069-7