Dissociation kinetics of hydrogen-passivated Pb defects at the (111)Si/SiO2 interface

被引:113
作者
Stesmans, A [1 ]
机构
[1] Katholieke Univ Leuven, Dept Phys, B-3001 Louvain, Belgium
来源
PHYSICAL REVIEW B | 2000年 / 61卷 / 12期
关键词
D O I
10.1103/PhysRevB.61.8393
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An electron-spin-resonance study has been carried out, both isothermally and isochronically, of the recovery under vacuum annealing from the hydrogen passivated state (symbolized as HPb) of paramagnetic P-b centers (Si(3)equivalent to Si-.) at the (111)Si/SiO2 interface. Previous work had reported simple exponential decay of [PbH] vs time, taken as key evidence for the process obeying the first-order rate equation d[PbH]/dt = -k(d)[PbH], where k(d)=k(do) exp(-E-d/kT) and E-d the single-valued activation energy. This inference, however, suffered from inadequate data. In contrast, experimental upgrading reveals manifest nonsimple exponential decay, which, within the simple thermal model, reveals the existence of a distinct spread sigma(Ed) in E-d Incorporation of Gaussian spread in E-d leads to a consistent generalized simple thermal model, that matches physical insight. The broad range of data enabled unbiased determination of the physical parameters involved, giving E-d = 2.83 +/- 0.02 eV, sigma(Ed) = 0.08 +/- 0.03 eV, and attempt frequency k(do) = (1.6+/-0.5) X 10(13) s(-1), close to the Si-H waging mode frequency, which provides a clue to the atomic dissociation mechanism. The spread sigma(Ed) results from the interfacial stress-induced Variations in P-b defect morphology. The body of data is found incompatible with second-order kinetics, thus exposing PbH dissociation as an individual process. Combination with the previous generalized thermal model for P-b passivation with H-2 culminates in a consistent unified picture of the P-b-hydrogen interaction kinetics.
引用
收藏
页码:8393 / 8403
页数:11
相关论文
共 47 条
[1]   OXYGEN PRECIPITATION IN SILICON [J].
BORGHESI, A ;
PIVAC, B ;
SASSELLA, A ;
STELLA, A .
JOURNAL OF APPLIED PHYSICS, 1995, 77 (09) :4169-4244
[2]   DISSOCIATION KINETICS OF HYDROGEN-PASSIVATED (111) SI-SIO2 INTERFACE DEFECTS [J].
BROWER, KL .
PHYSICAL REVIEW B, 1990, 42 (06) :3444-3453
[3]   KINETICS OF H-2 PASSIVATION OF PB CENTERS AT THE (111) SI-SIO2 INTERFACE [J].
BROWER, KL .
PHYSICAL REVIEW B, 1988, 38 (14) :9657-9666
[4]   STRAIN BROADENING OF THE DANGLING-BOND RESONANCE AT THE (111)SI-SIO2 INTERFACE [J].
BROWER, KL .
PHYSICAL REVIEW B, 1986, 33 (07) :4471-4478
[5]   CHEMICAL-KINETICS OF HYDROGEN AND (111) SI-SIO2 INTERFACE DEFECTS [J].
BROWER, KL ;
MYERS, SM .
APPLIED PHYSICS LETTERS, 1990, 57 (02) :162-164
[6]   DEFECTS AND IMPURITIES IN THERMAL OXIDES ON SILICON [J].
BROWER, KL ;
LENAHAN, PM ;
DRESSENDORFER, PV .
APPLIED PHYSICS LETTERS, 1982, 41 (03) :251-253
[7]   SI-SIO2 FAST INTERFACE STATE MEASUREMENTS [J].
BROWN, DM ;
GRAY, PV .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1968, 115 (07) :760-+
[8]   TIME-RESOLVED ANNEALING OF INTERFACE TRAPS AT THE SILICON OXIDE-SILICON INTERFACE [J].
BURTE, EP .
JOURNAL OF APPLIED PHYSICS, 1988, 64 (10) :5013-5019
[9]   PASSIVATION AND DEPASSIVATION OF SILICON DANGLING BONDS AT THE SI/SIO2 INTERFACE BY ATOMIC-HYDROGEN [J].
CARTIER, E ;
STATHIS, JH ;
BUCHANAN, DA .
APPLIED PHYSICS LETTERS, 1993, 63 (11) :1510-1512
[10]   LOW-TEMPERATURE REDUCTION OF FAST SURFACE STATES ASSOCIATED WITH THERMALLY OXIDIZED SILICON [J].
CASTRO, PL ;
DEAL, BE .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1971, 118 (02) :280-+