Expansion and shrinkage of the sulfur composite electrode in rechargeable lithium batteries

被引:156
作者
He, Xiangming [1 ]
Ren, Jianguo [1 ]
Wang, Li [1 ]
Pu, Weihua [1 ]
Jiang, Changyin [1 ]
Wan, Chunrong [1 ]
机构
[1] Tsinghua Univ, Inst Nucl & New Energy Technol, Beijing 100084, Peoples R China
关键词
Sulfur composite cathode; Rechargeable lithium batteries; Electrode expansion and shrinkage; CATHODE MATERIALS; CHARGE/DISCHARGE CHARACTERISTICS; ION; INTERCALATION; CELLS; STORAGE; CYCLE;
D O I
10.1016/j.jpowsour.2008.07.034
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The expansion and shrinkage characteristics of sulfur composite cathode electrode in rechargeable lithium batteries have been investigated. It was found that the sulfur composites electrodes expanded when discharging and shrank when charging again. The thickness change of the electrode was measured to be about 22%. The thickness of lithium metal anodes was also changed when lithium deposition and dissolution, while the sulfur composites electrodes expanded and shrank conversely. The investigation showed that the thickness changes of lithium anode and sulfur composite cathode could be compensated with each other to keep the total thickness of the cell not to change so much. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:154 / 156
页数:3
相关论文
共 26 条
[1]   Li-insertion in hard carbon anode materials for Li-ion batteries. [J].
Buiel, E ;
Dahn, JR .
ELECTROCHIMICA ACTA, 1999, 45 (1-2) :121-130
[2]   Rechargeable lithium sulfur battery - I. Structural change of sulfur cathode during discharge and charge [J].
Cheon, SE ;
Ko, KS ;
Cho, JH ;
Kim, SW ;
Chin, EY ;
Kim, HT .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (06) :A796-A799
[3]   Rechargeable lithium sulfur battery - II. Rate capability and cycle characteristics [J].
Cheon, SE ;
Ko, KS ;
Cho, JH ;
Kim, SW ;
Chin, EY ;
Kim, HT .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (06) :A800-A805
[4]   DEPENDENCE OF THE ELECTROCHEMICAL INTERCALATION OF LITHIUM IN CARBONS ON THE CRYSTAL-STRUCTURE OF THE CARBON [J].
DAHN, JR ;
SLEIGH, AK ;
SHI, H ;
REIMERS, JN ;
ZHONG, Q ;
WAY, BM .
ELECTROCHIMICA ACTA, 1993, 38 (09) :1179-1191
[5]   Charge/discharge characteristics of sulfur composite electrode at different temperature and current density in rechargeable lithium batteries [J].
He, Xiangming ;
Pu, Weihua ;
Ren, Jianguo ;
Wang, Li ;
Wang, Jiulin ;
Jiang, Changyin ;
Wan, Chunrong .
IONICS, 2008, 14 (04) :335-337
[6]   Charge/discharge characteristics of sulfur composite cathode materials in rechargeable lithium batteries [J].
He, Xiangming ;
Pu, Weihua ;
Ren, Jianguo ;
Wang, Li ;
Wang, Jiulin ;
Jiang, Changyin ;
Wan, Chunrong .
ELECTROCHIMICA ACTA, 2007, 52 (25) :7372-7376
[7]   Battery dimensional changes occurring during charge/discharge cycles - thin rectangular lithium ion and polymer cells [J].
Lee, JH ;
Lee, HM ;
Ahn, S .
JOURNAL OF POWER SOURCES, 2003, 119 :833-837
[8]   Design and characteristics of large-scale lithium ion battery [J].
Majima, M ;
Tada, T ;
Ujiie, S ;
Yagasaki, E ;
Inazawa, S ;
Miyazaki, K .
JOURNAL OF POWER SOURCES, 1999, 81 :877-881
[9]   Development of 1 kWh (300 Ah) class lithium-ion battery [J].
Majima, M ;
Hanafusa, K ;
Oka, Y ;
Tanaka, G ;
Yoshida, H ;
Yagasaki, E ;
Tada, T .
JOURNAL OF POWER SOURCES, 1997, 68 (02) :448-450
[10]   Electrochemical performance of lithium/sulfur cells with three different polymer electrolytes [J].
Marmorstein, D ;
Yu, TH ;
Striebel, KA ;
McLarnon, FR ;
Hou, J ;
Cairns, EJ .
JOURNAL OF POWER SOURCES, 2000, 89 (02) :219-226