Ultrafine fibrous cellulose membranes from electrospinning of cellulose acetate

被引:528
作者
Liu, HQ [1 ]
Hsieh, YL [1 ]
机构
[1] Univ Calif Davis, Davis, CA 95616 USA
关键词
electrospinning; cellulose; solution properties; viscosity; fibers; hydrolysis;
D O I
10.1002/polb.10261
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Three solvents, that is, acetone, acetic acid, and dimethylacetamide (DMAc), with a range of solubility parameter delta, surface tension gamma, viscosity eta and boiling temperature were used to generate mixtures for electrospinning cellulose acetate (CA) (degree of substitution, DS=2.45). Although none of these solvents alone enables continuous formation of fibers, mixing DMAc with either acetone or acetic acid produced suitable solvent systems. The 2:1 acetone:DMAc mixture is the most versatile mixture because it allows CA in the 12.5-20% concentration range to be continuously electrospun into fibrous membranes. These CA solutions have eta between 1.2 and 10.2 poise and gamma around 26 dyne/cm and produce smooth fibers with diameters from 100 nm to similar to1 mum. Fiber sizes generally decrease with decreasing CA concentrations. The nature of the collectors affects the morphology as well as packing of fibers. Fibers collected on paper have more uniform sizes, smooth surfaces, and fewer defects, whereas fibers collected on water are more varied in size. Electrically conductive solid collectors, such as Al foil and water, favor more tightly packed and less porous membranes. Porous collectors, like paper and copper mesh, produce highly porous membranes. The pores in membranes collected on the Al foil and paper are much better interconnected in the planar directions than those in membranes collected on water. There is evidence that electrospinning induces order in the fibers. Deacetylation of CA membranes is more efficient and complete in NaOH/ethanol than in aqueous NaOH, producing DS values between 0.15 and 2.33 without altering fiber surfaces, packing, or organization. The fully regenerated cellulose membranes are similarly hydrophilic as commodity cellulose fibrous matrices but absorb nearly 10 times as much water. (C) 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 2119-2129, 2002.
引用
收藏
页码:2119 / 2129
页数:11
相关论文
共 23 条
  • [1] Bergshoef MM, 1999, ADV MATER, V11, P1362, DOI 10.1002/(SICI)1521-4095(199911)11:16<1362::AID-ADMA1362>3.0.CO
  • [2] 2-X
  • [3] BRANDRUP J, 1989, POLYM HDB, P29
  • [4] Processing and microstructural characterization of porous biocompatible protein polymer thin films
    Buchko, CJ
    Chen, LC
    Shen, Y
    Martin, DC
    [J]. POLYMER, 1999, 40 (26) : 7397 - 7407
  • [5] Controlled deposition of electrospun poly(ethylene oxide) fibers
    Deitzel, JM
    Kleinmeyer, JD
    Hirvonen, JK
    Tan, NCB
    [J]. POLYMER, 2001, 42 (19) : 8163 - 8170
  • [6] Edgar K. J., 1998, ACS SYM SER, V688, P38
  • [7] Beaded nanofibers formed during electrospinning
    Fong, H
    Chun, I
    Reneker, DH
    [J]. POLYMER, 1999, 40 (16) : 4585 - 4592
  • [8] FONG H, 2000, STRUCTURE FORMATION, P225
  • [9] LIQUID TRANSPORT IN FABRIC STRUCTURES
    HSIEH, YL
    [J]. TEXTILE RESEARCH JOURNAL, 1995, 65 (05) : 299 - 307
  • [10] Wetting, pore structure, and liquid retention of hydrolyzed polyester fabrics
    Hsieh, YL
    Miller, A
    Thompson, J
    [J]. TEXTILE RESEARCH JOURNAL, 1996, 66 (01) : 1 - 10