Failure detection and monitoring in polymer matrix composites subjected to static and dynamic loads using carbon nanotube networks

被引:99
作者
Nofar, M. [1 ]
Hoa, S. V. [1 ]
Pugh, M. D. [1 ]
机构
[1] Concordia Univ, CREPEC, Concordia Ctr Composites, Dept Mech & Ind Engn, Montreal, PQ H3G 2W1, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Polymer composites; Carbon nanotubes; Electrical properties; Sensors; Nanocomposites; Smart materials; Fatigue; STRAIN; DAMAGE; MECHANICS; STRENGTH; SENSORS;
D O I
10.1016/j.compscitech.2009.03.010
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this work, multiwall carbon nanotubes (MWCNTs) have been used as a network of sensors to predict the failure region and to monitor the degradation of mechanical properties in laminated composites subjected to tensile and cyclic fatigue loadings. This is achieved by measuring the electrical resistance change in the semi-conductive MWCNT-fiber glass-epoxy polymer matrix composites. By partitioning the tensile and fatigue samples with electrically conductive probes, it is shown that with both increasing tensile load and number of cycles different resistance changes are detected in different regions and failure happens in the part in which higher resistance change was detected. In cyclic loading, when compared to strain gauge readings, resistance change measurements show more sensitivity in identifying the crack location, which gives this technique a good potential for monitoring damage during fatigue. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1599 / 1606
页数:8
相关论文
共 22 条
  • [1] Load and health monitoring in glass fibre reinforced composites with an electrically conductive nanocomposite epoxy matrix
    Boeger, Lars
    Wichmann, Malte H. G.
    Meyer, Leif Ole
    Schulte, Karl
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (7-8) : 1886 - 1894
  • [2] Chou T.-W., 1992, MICROSTRUCTURAL DESI
  • [3] Nanotube film based on single-wall carbon nanotubes for strain sensing
    Dharap, P
    Li, ZL
    Nagarajaiah, S
    Barrera, EV
    [J]. NANOTECHNOLOGY, 2004, 15 (03) : 379 - 382
  • [4] Bending and buckling of carbon nanotubes under large strain
    Falvo, MR
    Clary, GJ
    Taylor, RM
    Chi, V
    Brooks, FP
    Washburn, S
    Superfine, R
    [J]. NATURE, 1997, 389 (6651) : 582 - 584
  • [5] GIANG TP, 2008, COMPOSITES B, V39, P209
  • [6] Structural flexibility of carbon nanotubes
    Iijima, S
    Brabec, C
    Maiti, A
    Bernholc, J
    [J]. JOURNAL OF CHEMICAL PHYSICS, 1996, 104 (05) : 2089 - 2092
  • [7] Non-destructive testing of FRP by d.c. and a.c. electrical methods
    Kupke, M
    Schulte, K
    Schüler, R
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2001, 61 (06) : 837 - 847
  • [8] A structural mechanics approach for the analysis of carbon nanotubes
    Li, CY
    Chou, TW
    [J]. INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2003, 40 (10) : 2487 - 2499
  • [9] Carbon nanotube film sensors
    Li, ZL
    Dharap, P
    Nagarajaiah, S
    Barrera, EV
    Kim, JD
    [J]. ADVANCED MATERIALS, 2004, 16 (07) : 640 - +
  • [10] ELECTRONIC AND STRUCTURAL-PROPERTIES OF CARBON NANOTUBES
    MINTMIRE, JW
    WHITE, CT
    [J]. CARBON, 1995, 33 (07) : 893 - 902