Degradation study of MEA for PEMFCs under low humidity conditions

被引:280
作者
Endoh, E [1 ]
Terazono, S [1 ]
Widjaja, H [1 ]
Takimoto, Y [1 ]
机构
[1] Asahi Glass Co Ltd, Res Ctr, Kanagawa Ku, Yokohama, Kanagawa 221, Japan
关键词
D O I
10.1149/1.1739314
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The degradation study of the membrane electrode assembly (MEA) for proton exchange membrane fuel cells (PEMFCs) under low humidity conditions was conducted. The MEA degradation was observed during low humidity open-circuit voltage tests. To investigate the degradation mechanism, we conducted electron spin resonance studies of the degenerated MEA, and confirmed the formation of radicals in the catalyst layers. The MEA degradation mechanism that includes the radical formation reaction was verified. (C) 2004 The Electrochemical Society.
引用
收藏
页码:A209 / A211
页数:3
相关论文
共 9 条
  • [1] ESR STUDY OF ACTIVATED CARBON-FIBERS - PRELIMINARY-RESULTS
    DIVITTORIO, SL
    NAKAYAMA, A
    ENOKI, T
    DRESSELHAUS, MS
    ENDO, M
    SHINDO, N
    [J]. JOURNAL OF MATERIALS RESEARCH, 1993, 8 (09) : 2282 - 2287
  • [2] ESR IN HEAT-TREATED CARBONS FROM THE ENDOCARP OF BABASSU COCONUT
    EMMERICH, FG
    RETTORI, C
    LUENGO, CA
    [J]. CARBON, 1991, 29 (03) : 305 - 311
  • [3] ENDOH E, 2002, EL SOC M ABSTR
  • [4] Mapping the structure of a non-native state of staphylococcal nuclease
    Ermacora, MR
    Ledman, DW
    Fox, RO
    [J]. NATURE STRUCTURAL BIOLOGY, 1996, 3 (01): : 59 - 66
  • [5] KINOSHITA K, 1988, CARBON ELECTROCHEMIC, P86
  • [6] LaConti A.B., 2003, HDB FUEL CELLS FUNDA, V3
  • [7] Peña JM, 2001, POLYM DEGRAD STABIL, V71, P153
  • [8] *SAN EL CO LTD, 2002, NEDO REP