Test results of the 100 kWh SMES model coil - AC loss performance

被引:17
作者
Hamajima, T
Hanai, S
Wachi, Y
Kyoto, M
Shimada, M
Ono, M
Shimada, K
Kushida, L
Tezuka, M
Martovetsky, N
Zbasnik, J
Moller, J
Hirano, N
Shinoda, K
Yamamoto, M
Takano, I
Himeno, T
Satow, T
机构
[1] Yamaguchi Univ, Ube, Yamaguchi 7558611, Japan
[2] Toshiba Corp, Tsurumi Ku, Yokohama, Kanagawa 2300045, Japan
[3] Univ Calif Lawrence Livermore Natl Lab, Livermore, CA 94550 USA
[4] Chubu Elect Power Co Inc, Midori Ku, Nagoya, Aichi 4598001, Japan
[5] Int Superconduct Technol Ctr, Minato Ku, Tokyo 1050004, Japan
[6] Natl Inst Fus Sci, Gifu 5095292, Japan
关键词
SMES; AC losses; cable-in-conduit conductors; forced flow;
D O I
10.1016/S0011-2275(99)00127-7
中图分类号
O414.1 [热力学];
学科分类号
摘要
In order to establish a technology needed for a small-scale 100 kWh SMES device, an SMES model coil was fabricated. Performance tests were carried out at the Japan Atomic Energy Research Institute (JAERI) in 1996. After that, the coil was installed in the Lawrence Livermore National Laboratory (LLNL) facility and tested in 1998, in collaboration between Japan and the United States. The AC losses measured at LLNL were in good agreement with those measured at JAERI. It was reconfirmed that the coupling loss of the coil could be expressed in two components: one with a short and another with a long coupling time constant, We found out from the Hall probe signals that the loop currents with long decay times were induced in the CIC conductor by varying magnetic field. These currents resulted in additional AC loss in the coil. To develop a concept of CIC with low AC loss, we made a sub-scale CIC conductor of strands coated with CuNi. We fabricated a small coil out of this conductor and measured the AC loss. The measured AC loss in this coil was about 1/6 of that in the SMES model coil conductor per strand volume. Thus, the CuNi coating of the strands was demonstrated to be effective to reduce the AC loss in the coil. (C) 2000 Cryogenic Association of Japan, Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:947 / 953
页数:7
相关论文
共 22 条
[1]  
FUNAKI K, 1995, MULTIFILAMENTARY WIR
[2]  
HAMADA K, 1998, CRYOGENIC ENG, V33, P467
[3]   Test results of the SMES model coil-pulse performance [J].
Hamajima, T ;
Shimada, M ;
Ono, M ;
Takigami, H ;
Hanai, S ;
Wachi, Y ;
Takahashi, Y ;
Matui, K ;
Ito, T ;
Isono, T ;
Tsuji, H ;
Shinoda, K ;
Minemura, T ;
Himeno, T ;
Takano, I ;
Satow, T .
CRYOGENICS, 1999, 39 (04) :351-357
[4]  
HANAI S, 1998, CRYOGENIC ENG, V33, P460
[5]  
ISONO T, 1998, CRYOG ENG, V33, P473
[6]  
ITO S, 1998, CRYOGENIC ENG, V33, P485
[7]   Ramp-rate limitation experiments using a hybrid superconducting cable [J].
Jeong, S ;
Schultz, JH ;
Takayasu, M ;
Vysotsky, V ;
Michael, PC ;
Warnes, W ;
Shen, S .
CRYOGENICS, 1996, 36 (08) :623-629
[8]   Ramp-rate limitation due to current imbalance in a large cable-in-conduit conductor consisting of chrome-plated strands [J].
Koizumi, N ;
Takahashi, Y ;
Nishi, M ;
Isono, T ;
Tsuji, H ;
Ono, M ;
Hamajima, T ;
Fujioka, T .
CRYOGENICS, 1997, 37 (08) :441-452
[9]   Superconducting storage systems: An overview [J].
Luongo, CA .
IEEE TRANSACTIONS ON MAGNETICS, 1996, 32 (04) :2214-2223
[10]  
Masada E., 1994, P IEA S US SUP EN ST, P97