Residual stresses, strength and toughness of laminates with different layer thickness ratios

被引:125
作者
Bermejo, R.
Torres, Y.
Sanchez-Herencia, A. J.
Baudin, C.
Anglada, M.
Llanes, L.
机构
[1] Univ Politecn Cataluna, Dept Ciencia Mat & Ingn Met, ETSEIB, E-08028 Barcelona, Spain
[2] CSIC, Inst Ceram & Vidrio, E-28049 Madrid, Spain
关键词
multilayers; residual stresses; fracture; threshold strength; toughness;
D O I
10.1016/j.actamat.2006.06.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of residual stresses on the strength, toughness and work of fracture of Al2O3-5 wt.% tZrO(2)/Al2O3-30 wt.% mZrO(2) layered ceramics with different thickness ratios has been investigated. The laminates, as well as a monolithic Al2O3-5 wt.% tZrO(2) used as reference material, were fabricated by sequential slip casting. Residual stresses were estimated experimentally using indentation techniques and analytically using a three-dimensional finite element model. Flexural strength was evaluated by means of four-point bending tests on specimens with natural and artificial (indentation) flaws. Experimental findings show the existence of a threshold strength in the laminates whose value depends on the layer thickness ratio. Crack growth resistance behaviour was studied by crack opening displacement-controlled tests and by recourse to a weight function analytical approach. The high compressive stresses in the internal layers yield a pronounced R-curve behaviour in the laminates. Regarding work of fracture, it is found to be enhanced to levels up to about six times that of the reference monolith. The results are discussed in terms of the optimum layered architectural design for structural applications on the basis of the compromise between threshold strength and energy absorption capability associated with crack bifurcation mechanisms occurring at fracture. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd, All rights reserved.
引用
收藏
页码:4745 / 4757
页数:13
相关论文
共 46 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]  
BARATTA FI, 1981, J AM CERAM SOC, V64, pC3, DOI 10.1111/j.1151-2916.1981.tb09533.x
[3]  
BARATTA FI, 1978, J AM CERAM SOC, V61, P90
[4]   Threshold strength evaluation on an Al2O3-ZrO2 multilayered system [J].
Bermejo, R. ;
Torres, Y. ;
Baudin, C. ;
Sanchez-Herencia, A. J. ;
Pascual, J. ;
Anglada, M. ;
Llanes, L. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) :1443-1448
[5]  
Bermejo R, 2006, FATIGUE FRACT ENG M, V29, P71, DOI [10.1111/j.1460-2695.2006-00962.x, 10.1111/j.1460-2695.2006.00962.x]
[6]   Thermal shock behavior of an Al2O3/ZrO2 multilayered ceramic with residual stresses due to phase transformations [J].
Bermejo, R ;
Llanes, L ;
Anglada, M ;
Supancic, P ;
Lube, T .
FRACTOGRAPHY OF ADVANCED CERAMICS II, 2005, 290 :191-198
[7]  
BERMEJO R, UNPUB COMP SCI TECH
[8]   Fracture variability and R-curve behavior in yttria-stabilized zirconia ceramics [J].
Casellas, D ;
Alcalá, J ;
Llanes, L ;
Anglada, M .
JOURNAL OF MATERIALS SCIENCE, 2001, 36 (12) :3011-3025
[9]   LAMINAR CERAMIC COMPOSITES [J].
CHARTIER, T ;
MERLE, D ;
BESSON, JL .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1995, 15 (02) :101-107
[10]   A SIMPLE WAY TO MAKE TOUGH CERAMICS [J].
CLEGG, WJ ;
KENDALL, K ;
ALFORD, NM ;
BUTTON, TW ;
BIRCHALL, JD .
NATURE, 1990, 347 (6292) :455-457