Nanotubes from the self-assembly of asymmetric crystalline-coil poly(ferrocenylsilane-siloxane) block copolymers

被引:211
作者
Raez, J [1 ]
Manners, I [1 ]
Winnik, MA [1 ]
机构
[1] Univ Toronto, Dept Chem, Toronto, ON M6S 3H6, Canada
关键词
D O I
10.1021/ja020349h
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Block copolymers with a high asymmetry normally give spherical starlike micelles in a solvent selective for the longer block. We have discovered that samples of poly(ferrocenyldimethylsilane-b-dimethylsiloxane) (PFS-b-PDMS) with block ratios of 1:12 form nanotubes in n-hexane and n-decane, which are poor solvents for PFS. Two block copolymer samples PFS40-b-PDMS480 (M-n = 45 300, PDI = 1.01) and PFS80-b-PDMS960 (M-n = 90 500, PDI = 1.01) were synthesized by sequential anionic polymerization. When self-assembly occurs, the PFS blocks aggregate and crystallize to form a shell with a cavity in the middle of the tube, while the PDMS blocks form the Corona. The nature of these structures was elucidated by conventional transmission electron microscopy and dark-field scanning transmission electron microscopy. Time- and temperature-dependence studies revealed that a variety of morphologies are formed initially depending on the conditions of sample preparation, but most of them eventually rearrange to form nanotubules. The lengths of the tubes can be varied with time and with the choice of solvents. We have been able to grow nanotubes with lengths reaching 0.1 mm. The presence of the hollow core was confirmed by trapping tetrabutyllead in the cavity and performing energy-dispersive X-ray measurements on the resulting structure.
引用
收藏
页码:10381 / 10395
页数:15
相关论文
共 64 条
[1]  
Alexandridis P., 2000, AMPHIPHILIC BLOCK CO
[2]   THERMODYNAMICS OF POLYDIMETHYLSILOXANE SOLUTIONS [J].
CHAHAL, RS ;
KAO, WP ;
PATTERSO.D .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS I, 1973, 69 (10) :1834-1848
[3]   Ordered bicontinuous nanoporous and nanorelief ceramic films from self assembling polymer precursors [J].
Chan, VZH ;
Hoffman, J ;
Lee, VY ;
Iatrou, H ;
Avgeropoulos, A ;
Hadjichristidis, N ;
Miller, RD ;
Thomas, EL .
SCIENCE, 1999, 286 (5445) :1716-1719
[4]   Solubilization and encapsulation of fullerenes by amphiphilic block copolymers [J].
Chen, XL ;
Jenekhe, SA .
LANGMUIR, 1999, 15 (23) :8007-8017
[5]   Structure of poly(ferrocenyldimethylsilane) in electrospun nanofibers [J].
Chen, ZH ;
Foster, MD ;
Zhou, WS ;
Fong, H ;
Reneker, DH ;
Resendes, R ;
Manners, I .
MACROMOLECULES, 2001, 34 (18) :6156-6158
[6]   Helical superstructures from charged poly(styrene)-poly(isocyanodipeptide) block copolymers [J].
Cornelissen, JJLM ;
Fischer, M ;
Sommerdijk, NAJM ;
Nolte, RJM .
SCIENCE, 1998, 280 (5368) :1427-1430
[7]  
DEGENNES PG, 1987, CR ACAD SCI II, V304, P259
[8]   Hairy, semi-shaved, and fully shaved hollow nanospheres from polyisoprene block poly(2-cinnamoylethyl methacrylate) [J].
Ding, JF ;
Liu, GJ .
CHEMISTRY OF MATERIALS, 1998, 10 (02) :537-542
[9]   Polymer vesicles in various media [J].
Discher, BM ;
Hammer, DA ;
Bates, FS ;
Discher, DE .
CURRENT OPINION IN COLLOID & INTERFACE SCIENCE, 2000, 5 (1-2) :125-131
[10]  
DROSCHER M, 1982, MACROMOLECULES, V15, P442