FTIR spectroscopy of alcohol and formate interactions with mesoporous TiO2 surfaces

被引:41
作者
Brownson, Jeffrey R. S.
Tejedor-Tejedor, M. Isabel
Anderson, Marc A.
机构
[1] Univ Wisconsin, Environm Chem & Technol Program, Madison, WI 53706 USA
[2] CNRS, Inst Sci Chim Seine Amont, F-94320 Thiais, France
关键词
D O I
10.1021/jp0614547
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of pH and ultraviolet (UV) light with ligated formic acid on mesoporous TiO2 were characterized by transmission Fourier transform infrared (FTIR) spectroscopy and compared with adsorbed formate complexes. Surface-modified anatase thin films were prepared from acidic aqueous nanoparticulate anatase suspensions diluted with methanol and ethanol. Bands assigned to carboxylic acid groups displayed unique bonding character in the ligated formic acid on the anatase surface. For increased proton concentrations in the films, separation in -COO stretching bands (Delta nu) for formic acid increased (increase in frequency for nu C=O and decrease in frequency for nu C-O). With UV exposure, surface-bound organics were rapidly removed by photocatalytic oxidation at 40 degrees C and 40% relative humidity (RH). In addition, the Delta nu of the formic acid bands decreased as organics were mineralized to carbonates and CO2 with UV light. Aqueous formic acid adsorption experiments showed a distinctly different bonding environment lacking carbonate, and the Delta nu for the carboxylic groups indicated a bridging bidentate coordination. The Delta nu of the bands increased with increasing proton concentration, with both bands shifting to higher wavenumbers. The shifts may be ascribed to the influence of protonation on surface charge and the effect of that charge on the electronegativity of carboxylate groups bound to the surface. As alcohols are used in the mesoporous TiO2 solar cell preparation, implications of these surface modifications to dye-sensitized photovoltaics are discussed.
引用
收藏
页码:12494 / 12499
页数:6
相关论文
共 21 条
  • [1] [Anonymous], 1992, INTERMOLECULAR SURFA
  • [2] Photoreactive anatase consolidation characterized by FTIR Spectroscopy
    Brownson, JRS
    Tejedor-Tejedor, MI
    Anderson, MA
    [J]. CHEMISTRY OF MATERIALS, 2005, 17 (25) : 6304 - 6310
  • [3] Surface re-esterification and photo sintering of titania xerogel thin films
    Brownson, JRS
    Lee, TJ
    Anderson, MA
    [J]. CHEMISTRY OF MATERIALS, 2005, 17 (11) : 3025 - 3030
  • [4] The sol-gel transformation of TIPT coatings: a FTIR study
    Burgos, M
    Langlet, M
    [J]. THIN SOLID FILMS, 1999, 349 (1-2) : 19 - 23
  • [5] INFRARED SPECTROSCOPIC IDENTIFICATION OF SPECIES ARISING FROM REACTIVE ADSORPTION OF CARBON OXIDES ON METAL-OXIDE SURFACES
    BUSCA, G
    LORENZELLI, V
    [J]. MATERIALS CHEMISTRY, 1982, 7 (01): : 89 - 126
  • [6] Infrared reflectivity and lattice fundamentals in anatase TiO2
    Gonzalez, RJ
    Zallen, R
    Berger, H
    [J]. PHYSICAL REVIEW B, 1997, 55 (11) : 7014 - 7017
  • [7] Gratzel M, 1991, NATURE, V353, P737, DOI DOI 10.1038/53737A0
  • [8] Interfacial recombination processes in dye-sensitized solar cells and methods to passivate the interfaces
    Gregg, BA
    Pichot, F
    Ferrere, S
    Fields, CL
    [J]. JOURNAL OF PHYSICAL CHEMISTRY B, 2001, 105 (07) : 1422 - 1429
  • [9] A system approach to molecular solar cells
    Hagfeldt, A
    Boschloo, G
    Lindström, H
    Figgemeier, E
    Holmberg, A
    Aranyos, V
    Magnusson, E
    Malmqvist, L
    [J]. COORDINATION CHEMISTRY REVIEWS, 2004, 248 (13-14) : 1501 - 1509
  • [10] FTIR study of adsorption and photoassisted oxygen isotopic exchange of carbon monoxide, carbon dioxide, carbonate, and formate on TiO2
    Liao, LF
    Lien, CF
    Shieh, DL
    Chen, MT
    Lin, JL
    [J]. JOURNAL OF PHYSICAL CHEMISTRY B, 2002, 106 (43) : 11240 - 11245