Bond strength to primed Ti-6Al-7Nb alloy of two acrylic resin adhesives

被引:19
作者
Koizumi, Hiroyasu
Furuchi, Mika
Tanoue, Naomi
Yanagida, Hiroaki
Yoneyama, Takayuki
Matsumura, Hideo
机构
[1] Nihon Univ, Sch Dent, Dept Crown & Bridge Prosthodont, Chiyoda Ku, Tokyo 1018310, Japan
[2] Nihon Univ, Sch Dent, Dent Res Ctr, Div Adv Dent Treatment,Chiyoda Ku, Tokyo 1018310, Japan
[3] Nagasaki Univ, Hosp Med & Dent, Dept Specialized Dent, Nagasaki 8528588, Japan
[4] Tokyo Med & Dent Univ, Inst Biomat & Bioengn, Dept Met, Chiyoda Ku, Tokyo 1010062, Japan
关键词
bonding; niobium; titanium;
D O I
10.4012/dmj.25.286
中图分类号
R78 [口腔科学];
学科分类号
1003 [口腔医学];
摘要
This study aimed to evaluate the bonding behavior of two acrylic resin adhesives joined to titanium-aluminum-niobium (Ti-6Al-7Nb) alloy primed with two metal conditioners. Cast Ti-6Al-7Nb alloy disks were air-abraded with alumina and bonded with six combinations of two resin adhesives (Super-Bond C&B and Multi Bond) and three surface conditions (Alloy Primer, M.L. Primer, and unprimed control). Shear bond strengths were determined both before and after 20,000 thermal cycles. The tri-n-butylborane initiated Super-Bond C&B resin exhibited greater bond strength than the BPC-amine initiated Multi-Bond resin. Both the Alloy Primer with a hydrophobic phosphate and the M.L. Primer with a phosphonoacetate effectively improved the 24-hour bond strength of Multi-Bond resin as well as the post-thermocycling bond.strength of Super-Bond C&B resin.
引用
收藏
页码:286 / 290
页数:5
相关论文
共 27 条
[1]
Titanium for removable partial dentures (III): 2-year clinical follow-up in an undergraduate programme [J].
Au, AR ;
Lechner, SK ;
Thomas, CJ ;
Mori, T ;
Chung, P .
JOURNAL OF ORAL REHABILITATION, 2000, 27 (11) :978-984
[2]
BERGMAN B, 1994, SWED DENT J, V18, P25
[3]
Titanium for removable denture bases [J].
Da Silva, L ;
Martinez, A ;
Rilo, B ;
Santana, U .
JOURNAL OF ORAL REHABILITATION, 2000, 27 (02) :131-135
[4]
ADHESION TO TITANIUM OF METHACRYLATE-BASED POLYMER MATERIALS [J].
EKSTRAND, K ;
RUYTER, IE ;
OYSAED, H .
DENTAL MATERIALS, 1988, 4 (03) :111-115
[5]
SHEAR BOND STRENGTH OF 4 COMMERCIAL BONDING SYSTEMS TO CPTI [J].
FUJISHIMA, A ;
FUJISHIMA, Y ;
FERRACANE, JL .
DENTAL MATERIALS, 1995, 11 (02) :82-86
[6]
HANSSON O, 1990, SCAND J DENT RES, V98, P248
[7]
HANSSON O, 1993, SCAND J DENT RES, V101, P243
[8]
Imai Y, 2003, REPORTS I BIOMATERIA, V37, P4
[9]
Effect of acidic primers on bonding three magnetic steel alloys with tri-n-butylborane initiated methacrylic resin [J].
Ishikawa, Y ;
Kawamoto, Y ;
Nemoto, M ;
Koizumi, H ;
Nemoto, K ;
Matsumura, H .
DENTAL MATERIALS JOURNAL, 2005, 24 (04) :642-647
[10]
Kern M, 1995, J Prosthodont, V4, P16, DOI 10.1111/j.1532-849X.1995.tb00309.x