Ni-Al-Ti coatings obtained by microwave assisted SHS: Effect of annealing on microstructural and mechanical properties

被引:32
作者
Cammarota, G. P. [1 ]
Casagrande, A. [1 ]
Poli, G.
Veronesi, P.
机构
[1] Univ Bologna, SMETEC, I-40126 Bologna, Italy
关键词
Coatings; Microwaves; Interlocking microstructure; Liquid phase bonding; SURFACE MODIFICATION; STRUCTURAL FORMATION; FRACTURE-TOUGHNESS; ALUMINIDE COATINGS; TITANIUM; RESISTANCE; CR;
D O I
10.1016/j.surfcoat.2008.11.017
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microwaves at 2.45 GHz have been used to ignite the self-propagating high-temperature synthesis (SHS) in a Ni and Al powder mixture to produce NiAl coatings on Ti. The temperature of the reacting powders, owing to the exothermic nature of the reaction and to the energy provided by the high frequency electromagnetic field, reaches the melting temperature of NiAl. The newly formed NiAl, in the liquid phase, reacts with the underlying Ti and rapidly forms at the interface a ternary eutectic belonging to the Ni-Al-Ti system. During cooling, the formed transient liquid eutectic layer at the Ti/NiAl interface originates an intermediate layer presenting an interlocking network, which constitutes an in-situ reinforcement phase. In this study it is shown that the thickness of the interface layer can be altered by annealing at temperature higher than the ternary eutectic temperature (904 degrees C), in a few minutes time. Experimental results demonstrated also that, due to its peculiar microstructure, the intermediate layer is tougher and harder than the parent NiAl coating. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:1429 / 1437
页数:9
相关论文
共 36 条
[1]  
Abson D. J., 1986, International Metals Reviews, V31, P141
[2]   Formation of dendritic structure in the diffusion zone of the bonded Zircaloy-4 and stainless steel 316L in the presence of Ti interlayer [J].
Akhter, JI ;
Ahmad, M ;
Iqbal, M ;
Akhtar, M ;
Shaikh, MA .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 399 (1-2) :96-100
[3]  
*ASM, 1992, ASM HDB ALL PHAS DIA, V3
[4]  
*ASM, 1994, ASM PUBLICATON
[5]   Titanium for aerospace: Rationale and applications [J].
Boyer, RR .
ADVANCED PERFORMANCE MATERIALS, 1995, 2 (04) :349-368
[6]   Effect of Ni, Si and Cr in the structural formation of diffusion aluminide coatings on commercial-purity titanium [J].
Cammarota, G. P. ;
Casagrande, A. ;
Sambogna, G. .
SURFACE & COATINGS TECHNOLOGY, 2006, 201 (1-2) :230-242
[7]   Effect of ternary additions of iron on microstructure and microhardness of the intermetallic NiAl in reactive sintering [J].
Cammarota, GP ;
Casagrande, A .
JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 381 (1-2) :208-214
[8]  
CAMMAROTA GP, 2007, EURO PM2007 P OCT 15, V3, P157
[9]  
CASAGRANDE A, 2005, EURO PM2005 P 2 5 OC, V1, P107
[10]  
Casagrande A., 2008, P EURO INT POWDER ME, V3, P71