A TEM investigation on indentation plastic zones in Ni3Al(Cr,B) single crystals

被引:109
作者
Chiu, YL [1 ]
Ngan, AHW [1 ]
机构
[1] Univ Hong Kong, Dept Mech Engn, Hong Kong, Hong Kong, Peoples R China
关键词
single crystal; nanoindentation; mechanical properties; yield phenomena;
D O I
10.1016/S1359-6454(02)00100-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Nanoindentation has been carried out on (111) single crystals of Ni3Al with the maximum applied load ranging from 800 to 8000 muN. The indentation plasticity fields are found to consist of two regions. namely, a core with a very high dislocation density and a surrounding region where the dislocation density is much lower. In the zone with lower dislocation density, individual dislocations were discernible, and three sets of dislocations, with Burgers vector of the <1 (1) over bar0> type and parallel to the sample surface, were identified in all specimens. The dislocation segments were curvy at small loads but long and straight screw dislocations appeared at large loads. Measurements of the radii of the plasticity zones from TEM images indicate that the core and the surrounding low dislocation density zone did not evolve in a self-similar manner with increasing load. From the dislocation structure observed just after the pop-in in the load-displacement curve, the strain rate in the indent core during pop-in is estimated to be about 170 s(-1). The nominal hardness calculated using the Oliver-Pharr scheme exhibits a sharp and negative dependence with respect to load. with the hardness dropping from similar to12 GPa at 800 muN to about 6 GPa at 8000 muN. The value of P/pic(2), where P is the load and c the radius of the surrounding dislocation zone, is however fairly constant with respect to load, with a variation of only about 10% in the same load range. The yield stress Y calculated from the equation Y = 1.5P/pic(2) is about 356 +/- 32 MPa. These results suggest that, while nanohardness can still be expected to depend critically on the yield stress, there is an additional functional relationship that causes the hardness to vary with the indent size in the submicron regime. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2677 / 2691
页数:15
相关论文
共 36 条
[1]   Plastic zone and pileup around large indentations [J].
Bahr, DF ;
Gerberich, WW .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (12) :3793-3800
[2]   Non-linear deformation mechanisms during nanoindentation [J].
Bahr, DF ;
Kramer, DE ;
Gerberich, WW .
ACTA MATERIALIA, 1998, 46 (10) :3605-3617
[3]   A transmission electron microscope study of hardness indentations in MoSi2 [J].
Boldt, PH ;
Weatherly, GC ;
Embury, JD .
JOURNAL OF MATERIALS RESEARCH, 2000, 15 (04) :1025-1032
[4]   A method for interpreting the data from depth-sensing indentation instruments [J].
Doerner, M. F. ;
Nix, W. D. .
JOURNAL OF MATERIALS RESEARCH, 1986, 1 (04) :601-609
[5]  
ESS SS, 1982, ACTA METALL, V30, P921
[6]   MICRO-HARDNESS OF METALS AT VERY LOW LOADS [J].
GANE, N ;
COX, JM .
PHILOSOPHICAL MAGAZINE, 1970, 22 (179) :881-+
[7]   MICROSCOPY AND MICROINDENTATION MECHANICS OF SINGLE-CRYSTAL FE-3 WT-PERCENT-SI .1. ATOMIC-FORCE MICROSCOPY OF A SMALL INDENTATION [J].
HARVEY, S ;
HUANG, H ;
VENKATARAMAN, S ;
GERBERICH, WW .
JOURNAL OF MATERIALS RESEARCH, 1993, 8 (06) :1291-1299
[8]  
Johnson K. L., 1987, CONTACT MECH
[9]   CORRELATION OF INDENTATION EXPERIMENTS [J].
JOHNSON, KL .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1970, 18 (02) :115-&
[10]   Yield strength predictions from the plastic zone around nanocontacts [J].
Kramer, D ;
Huang, H ;
Kriese, M ;
Robach, J ;
Nelson, J ;
Wright, A ;
Bahr, D ;
Gerberich, WW .
ACTA MATERIALIA, 1998, 47 (01) :333-343