Reliability and properties of ground Y-TZP-zirconia ceramics

被引:221
作者
Luthardt, RG
Holzhüter, M
Sandkuhl, O
Herold, V
Schnapp, JD
Kuhlisch, E
Walter, M
机构
[1] Dresden Univ Technol, Sch Dent, Dept Prosthet Dent, D-01307 Dresden, Germany
[2] Univ Jena, Tech Inst, D-07743 Jena, Germany
[3] Dresden Univ Technol, Dept Med Informat & Biometry, D-01307 Dresden, Germany
关键词
zirconia; grinding; strength; fracture toughness; CAD/CAM;
D O I
10.1177/154405910208100711
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Yttria-stabilized zirconia ceramics is a high-performance material with excellent biocompatibility and mechanical properties, which suggest its suitability for posterior fixed partial dentures. The hypothesis under examination is that the strength and reliability of Y-TZP zirconia ceramics are affected by the inner surface grinding of crowns, and vary with the grinding parameter. Flexural strength, surface roughness, and fracture toughness were determined on samples machined by face and peripheral grinding with varied feed velocities and cutting depths. Results have been compared with those on lapped samples. Analysis of variance and Weibull parameter were used for statistical analysis. It was found that inner surface grinding significantly reduces the strength and reliability of Y-TZP zirconia compared with the lapped control sample. Co-analysis of flexural strength, Weibull parameter, and fracture toughness showed counteracting effects of surface compressive stress and grinding-introduced surface flaws. In conclusion, grinding of Y-TZP needs to be optimized to achieve the CAD/CAM manufacture of all-ceramic restorations with improved strength and reliability.
引用
收藏
页码:487 / 491
页数:5
相关论文
共 11 条
[1]  
[Anonymous], INTCERAM
[2]  
*EN DIN, 1995, 8431 EN DIN
[3]  
Giordano R, 1995, Int J Prosthodont, V8, P311
[4]   The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic [J].
Kosmac, T ;
Oblak, C ;
Jevnikar, P ;
Funduk, N ;
Marion, L .
DENTAL MATERIALS, 1999, 15 (06) :426-433
[5]   Flexural strength of ceramics ground under widely different conditions [J].
Liao, TW ;
Li, K ;
Breder, K .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1997, 70 (1-3) :198-206
[6]  
LUTHARDT R, 1997, BIOCERAMICS, V10, P437
[7]   Evaluation of subsurface damage in CAD/CAM machined dental ceramics [J].
Sindel, J ;
Petschelt, A ;
Grellner, F ;
Dierken, C ;
Greil, P .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1998, 9 (05) :291-295
[8]  
STEVENS R, 1986, MAGNESIUM ELECT PUBL, V113
[9]   FRACTURE SURFACE CHARACTERIZATION OF CLINICALLY FAILED ALL CERAMIC CROWNS [J].
THOMPSON, JY ;
ANUSAVICE, KJ ;
NAMAN, A ;
MORRIS, HF .
JOURNAL OF DENTAL RESEARCH, 1994, 73 (12) :1824-1832
[10]  
Tinschert J, 2001, OPER DENT, V26, P367