摘要
The mechanisms of fatigue-crack propagation are examined with particular emphasis on the similarities and differences between cyclic crack growth in ductile materials, such as metals, and corresponding behavior in brittle materials, such as intermetallics and ceramics. This is achieved by considering the process of fatigue-crack growth as a mutual competition between intrinsic mechanisms of crack advance ahead of the crack tip (e.g., alternating crack-tip blunting and resharpening), which promote crack growth, and extrinsic mechanisms of crack-tip shielding behind the tip (e.g., crack closure and bridging), which impede it. The widely differing nature of these mechanisms in ductile and brittle materials and their specific dependence upon the alternating and maximum driving forces (e.g., Delta K and K-max) provide a useful distinction of the process of fatigue-crack propagation in different classes of materials; moreover, it provides a rationalization for the effect of such factors as load ratio and crack size. Finally, the differing susceptibility of ductile and brittle materials to cyclic degradation has broad implications for their potential structural application; this is briefly discussed with reference to lifetime prediction.
引用
收藏
页码:55 / 83
页数:29
相关论文
共 69 条
[1]  
[Anonymous], SHORT FATIGUE CRACKS
[2]  
[Anonymous], 1984, FATIGUE CRACK GROWTH
[3]  
[Anonymous], ASTM STP
[4]   FLOW CHARACTERISTICS OF HIGHLY CONSTRAINED METAL WIRES [J].
ASHBY, MF ;
BLUNT, FJ ;
BANNISTER, M .
ACTA METALLURGICA, 1989, 37 (07) :1847-1857
[5]   Fracture and fatigue-crack growth behavior in ductile-phase toughened molybdenum disilicide: Effects of niobium wire vs particulate reinforcements [J].
Badrinarayanan, K ;
McKelvey, AL ;
Rao, KTV ;
Ritchie, RO .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (12) :3781-3792
[6]  
Barenblatt G. I, 1961, Adv. Appl. Mech., P3, DOI DOI 10.1016/S0065-2156(08)70121-2
[7]   MICROSTRUCTURAL DESIGN OF TOUGHENED CERAMICS [J].
BECHER, PF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (02) :255-269
[8]   Resistance-curve toughening in ductile/brittle layered structures: Behavior in Nb/Nb3Al laminates [J].
Bloyer, DR ;
Rao, KTV ;
Ritchie, RO .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 216 (1-2) :80-90
[9]  
BLOYER DR, 1997, IN PRESS METALLURI A
[10]   On the growth of small fatigue cracks in gamma-based titanium aluminides [J].
Campbell, JP ;
Kruzic, JJ ;
Lillibridge, S ;
Rao, KTV ;
Ritchie, RO .
SCRIPTA MATERIALIA, 1997, 37 (05) :707-712