Characterization by solid state 51V NMR spectroscopy

被引:24
作者
Shubin, AA [1 ]
Lapina, OB [1 ]
Courcot, D [1 ]
机构
[1] Univ Littoral Coted Opal, MREID, Lab Catalyse & Environm, EA 2598, F-59140 Dunkerque, France
基金
俄罗斯基础研究基金会;
关键词
solid stare V-51 NMR; static and MAS experiments; SCR catalyst;
D O I
10.1016/S0920-5861(99)00298-9
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The fresh catalyst V2O5-WO3/TiO2 and catalyst used in SCR for 9000 h have been studied by the solid state V-51 NMR spectroscopy in static and MAS conditions. According to V-51 NMR in both samples the majority of vanadium sites are in a distorted octahedral environment similar to that in V2O5. There is a strong interaction between vanadium oxide and the support, but the concentration of vanadium atoms strongly bound to the surface is very small and can be detected only in MAS NMR experiments or after removing the excess of V2O5 There is no influence of WO3 additives on the structure of the particles of V2O5. whereas the influence on the structure of strongly bounded V cannot be excluded. Combination of static (wide line) and MAS NMR techniques permit the characterization of not only the structure of the vanadium species but also small changes in their local environment. Hence these experiments show that there are some distortions of the local environment of vanadium sites of the vanadium oxide particles compared with the polycrystalline V2O5; treatment by SCR increases these distortions. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:379 / 387
页数:9
相关论文
共 26 条
[1]   SIMULATION OF NMR POWDER SPECTRA [J].
AMOUREUX, JP ;
FERNANDEZ, C ;
CARPENTIER, L ;
COCHON, E .
PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1992, 132 (02) :461-475
[2]   Optimized multiple-quantum magic-angle spinning NMR experiments on half-integer quadrupoles [J].
Amoureux, JP ;
Fernandez, C ;
Frydman, L .
CHEMICAL PHYSICS LETTERS, 1996, 259 (3-4) :347-355
[3]   Two-dimensional MAS multiple-quantum NMR of quadrupolar nuclei, removal of inhomogeneous second-order broadening [J].
Brown, SP ;
Heyes, SJ ;
Wimperis, S .
JOURNAL OF MAGNETIC RESONANCE SERIES A, 1996, 119 (02) :280-284
[4]   FAST MAGIC-ANGLE-SPINNING SOLID-STATE V-51 NMR CHARACTERIZATION OF VANADIUM-OXIDE CATALYSTS SUPPORTED ON TIO2 [J].
COURCOT, D ;
BODART, P ;
FERNANDEZ, C ;
RIGOLE, M ;
GUELTON, M .
JOURNAL DE CHIMIE PHYSIQUE ET DE PHYSICO-CHIMIE BIOLOGIQUE, 1994, 91 (06) :909-915
[5]  
COURCOT D, 1996, J CHEM SOC FARADAY T, V92, P1607
[6]   PHYSICAL AND CHEMICAL CHARACTERIZATION OF SURFACE VANADIUM-OXIDE SUPPORTED ON TITANIA - INFLUENCE OF THE TITANIA PHASE (ANATASE, RUTILE, BROOKITE AND B) [J].
DEO, G ;
TUREK, AM ;
WACHS, IE ;
MACHEJ, T ;
HABER, J ;
DAS, N ;
ECKERT, H ;
HIRT, AM .
APPLIED CATALYSIS A-GENERAL, 1992, 91 (01) :27-42
[7]   PREDICTING MOLECULAR-STRUCTURES OF SURFACE METAL-OXIDE SPECIES ON OXIDE SUPPORTS UNDER AMBIENT CONDITIONS [J].
DEO, G ;
WACHS, IE .
JOURNAL OF PHYSICAL CHEMISTRY, 1991, 95 (15) :5889-5895
[8]   SOLID-STATE V-51 NMR STRUCTURAL STUDIES OF VANADIUM(V) OXIDE CATALYSTS SUPPORTED ON TIO2(ANATASE) AND TIO2(RUTILE) - THE INFLUENCE OF SURFACE IMPURITIES ON THE VANADIUM(V) COORDINATION [J].
ECKERT, H ;
DEO, G ;
WACHS, IE ;
HIRT, AM .
COLLOIDS AND SURFACES, 1990, 45 :347-359
[9]   SOLID-STATE V-15 NMR STRUCTURAL STUDIES ON SUPPORTED VANADIUM(V) OXIDE CATALYSTS - VANADIUM-OXIDE SURFACE-LAYERS ON ALUMINA AND TITANIA SUPPORTS [J].
ECKERT, H ;
WACHS, IE .
JOURNAL OF PHYSICAL CHEMISTRY, 1989, 93 (18) :6796-6805
[10]  
FERNANDEZ C, 1994, CATAL TODAY, V20, P77