Degradation of recycled high-impact polystyrene. Simulation by reprocessing and thermo-oxidation

被引:98
作者
Vilaplana, Francisco
Ribes-Greus, Amparo
Karlsson, Sigbritt
机构
[1] Royal Inst Technol, Dept Fibre & Polymer Technol, Sch Chem Sci & Engn, KTH, SE-10044 Stockholm, Sweden
[2] Univ Politecn Valencia, Inst Tecnol Mat, E-46022 Valencia, Spain
关键词
recycling; degree of degradation; high-impact polystyrene; reprocessing; thermo-oxidation;
D O I
10.1016/j.polymdegradstab.2006.01.007
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A simulation of the degradation of high-impact polystyrene (HIPS), occurring during service life and mechanical recycling, was performed by multiple processing and thermo-oxidative ageing. All samples were characterized by differential scanning calorimetry (DSC), melt mass-flow rate (MFR) measurements, tensile testing and infrared spectroscopy (FTIR). Multiple processing and thermo-oxidative ageing clearly alter the oxidative stability and the elongation at break of the materials. These changes observed at a macroscopic scale have been related to chemical alterations in the structure of HIPS. The polybutadiene phase was demonstrated to be the initiation point of the degradative processes induced by processing, service life and mechanical recycling. Thermo-oxidative degradation affects more severely the degree of degradation of the material, so it may be deduced that the changes occurring during service life of HIPS are the part of the life cycle that mostly affects its further recycling possibilities and performance in second-market applications. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2163 / 2170
页数:8
相关论文
共 17 条
[1]   Degradation of ABS during repeated processing and accelerated ageing [J].
Boldizar, A ;
Möller, K .
POLYMER DEGRADATION AND STABILITY, 2003, 81 (02) :359-366
[2]   Recycling of acrylonitrile-butadiene-styrene and high-impact polystyrene from waste computer equipment [J].
Brennan, LB ;
Isaac, DH ;
Arnold, JC .
JOURNAL OF APPLIED POLYMER SCIENCE, 2002, 86 (03) :572-578
[3]   ELEVATED-TEMPERATURE AGING OF HIPS [J].
CHEN, CC ;
HABIBULLAH, M ;
SAUER, JA .
JOURNAL OF APPLIED POLYMER SCIENCE, 1983, 28 (01) :391-406
[4]   Determination of the kinetic parameters of the thermal oxidative degradation of styrene/butadiene copolymers [J].
Grguric, TH ;
Rek, V ;
Jelcic, Z ;
Hace, D ;
Gomzi, Z .
POLYMER ENGINEERING AND SCIENCE, 1999, 39 (08) :1394-1397
[5]   PHOTOINITIATED AND THERMOINITIATED OXIDATION OF HIGH-IMPACT POLYSTYRENE .1. CHARACTERIZATION BY FT-IR SPECTROSCOPY [J].
ISRAELI, Y ;
LACOSTE, J ;
LEMAIRE, J ;
SINGH, RP ;
SIVRAM, S .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1994, 32 (03) :485-493
[6]  
Karlsson S, 2002, DEGRADABLE POLYMERS: PRINCIPLES AND APPLICATIONS, SECOND EDITION, P51
[7]   Recycled polyolefins. Material properties and means for quality determination [J].
Karlsson, S .
LONG-TERM PROPERTIES OF POLYOLEFINS, 2004, 169 :201-229
[8]   APPLICATION OF IR-COMPENSATION TECHNIQUE FOR STUDY OF THE OXIDATION DEGREE OF HIGH-IMPACT POLYSTYRENE [J].
KOSTOV, GI ;
KOMITOV, PG ;
NIKOLOVA, ZG .
EUROPEAN POLYMER JOURNAL, 1985, 21 (06) :561-564
[9]  
Lacoste J, 1996, J APPL POLYM SCI, V59, P953
[10]  
*PLAST EUR, 2004, PLAST EUR AN PLAST C