Thermochemical CO2 splitting reaction with supported LaxA1-xFeyB1-yO3 (A = Sr, Ce, B = Co, Mn; 0 ≤ x, y ≤ 1) perovskite oxides

被引:83
作者
Jiang, Qingqing [1 ,2 ]
Tong, Jinhui [1 ,2 ]
Zhou, Guilin [1 ,2 ]
Jiang, Zongxuan [1 ]
Li, Zhen [1 ,2 ]
Li, Can [1 ]
机构
[1] Chinese Acad Sci, Dalian Natl Lab Clean Energy, Dalian Inst Chem Phys, State Key Lab Catalysis, Dalian 116023, Peoples R China
[2] Chinese Acad Sci, Grad Univ, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
Solar energy; CO2; reduction; Perovskite oxide; Kinetics; SOLAR HYDROGEN-PRODUCTION; CATALYTIC-ACTIVITY; KINETIC-ANALYSIS; DISSOCIATION; WATER; COMBUSTION; OXIDATION; CYCLES; H2O; H-2;
D O I
10.1016/j.solener.2014.02.033
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
An efficient redox material for two-step thermochemical CO2 splitting reaction requires high chemical yield at relatively low reduction temperature. Herein, the oxides with perovskite structure of formula La(x)A(1-x)Fe(y)B(1-y)O(3) (A = Sr, Ce, B = Co, Mn; 0 <= x, y <= 1) start to release O-2 at 800 degrees C and the largest O-2 production is 11.8 ml/g(perovskite) at 1300 degrees C. However, for these unsupported La(x)A(1-x)Fe(y)B(1-y)O(3) materials, the CO production is low in spite of high reduction yield. ZrO2, Al2O3 and SiO2 are thus considered as supports to disperse La(x)A(1-x)Fe(y)B(1-y)O(3) materials and different supports induce great differences in the reaction activity. By A-site or B-site substitution of LaFeO3, the O-2 releasing temperature has fallen from 1230 degrees C to 800-950 degrees C and the CO production is enhanced 2-3 times. LaFe0.7Co0.3O3 (25 wt%)/SiO2 shows the highest reaction activity among these investigated materials with the O-2 production of 4.0 ml/g(material) (16.0 ml/g(perovskite)) and CO production of 7.6 ml/g(material) (30.4 ml/g(perovskite)) when it is reduced at 1300 degrees C and re-oxidized at 1100 degrees C, and the activity is relatively stable even after 10 cycles of the reaction. By contrast, the CO production is 4.5 ml/g for CeO2 when it is reduced at 1400 degrees C. The estimated activation energy for the reduction step of LaFe0.7Co0.3O3 (25 wt%)/SiO2 is around 89-149 KJ/mol according to different models. The CO generation step of LaFe0.7Co0.3O3 (25 wt%)/SiO2 is mainly controlled by bulk diffusion (D1) at 1000 degrees C and then it turns to first order surface reaction (F1) at 1100 degrees C. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:425 / 437
页数:13
相关论文
共 30 条
[1]   High-Flux Solar-Driven Thermochemical Dissociation of CO2 and H2O Using Nonstoichiometric Ceria [J].
Chueh, William C. ;
Falter, Christoph ;
Abbott, Mandy ;
Scipio, Danien ;
Furler, Philipp ;
Haile, Sossina M. ;
Steinfeld, Aldo .
SCIENCE, 2010, 330 (6012) :1797-1801
[2]   La(1-x)SrxMnO3-δ perovskites as redox materials for the production of high purity hydrogen [J].
Eudou, A. ;
Zaspalis, V. ;
Nalbandian, L. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2008, 33 (20) :5554-5562
[3]   Perovskite membrane reactor for continuous and isothermal redox hydrogen production from the dissociation of water [J].
Evdou, A. ;
Nalbandian, L. ;
Zaspalis, V. T. .
JOURNAL OF MEMBRANE SCIENCE, 2008, 325 (02) :704-711
[4]   Methane combustion on some perovskite-like mixed oxides [J].
Ferri, D ;
Forni, L .
APPLIED CATALYSIS B-ENVIRONMENTAL, 1998, 16 (02) :119-126
[5]   Manganese oxide dissociation kinetics for the Mn2O3 thermochemical water-splitting cycle. Part 1: Experimental [J].
Francis, Todd M. ;
Lichty, Paul R. ;
Weimer, Alan W. .
CHEMICAL ENGINEERING SCIENCE, 2010, 65 (12) :3709-3717
[6]   Solar hydrogen production by two-step thermochemical cycles: Evaluation of the activity of commercial ferrites [J].
Fresno, Fernando ;
Fernandez-Saavedra, Rocio ;
Belen Gomez-Mancebo, M. ;
Vidal, Alfonso ;
Sanchez, Miguel ;
Rucandio, M. Isabel ;
Quejido, Alberto J. ;
Romero, Manuel .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (07) :2918-2924
[7]   Syngas production by simultaneous splitting of H2O and CO2 via ceria redox reactions in a high-temperature solar reactor [J].
Furler, Philipp ;
Scheffe, Jonathan R. ;
Steinfeld, Aldo .
ENERGY & ENVIRONMENTAL SCIENCE, 2012, 5 (03) :6098-6103
[8]  
Galwey A.K., 1999, THERMAL DECOMPOSITIO, V1st
[9]   Kinetic analysis of solid-state reactions: The universality of master plots for analyzing isothermal and nonisothermal experiments [J].
Gotor, FJ ;
Criado, JM ;
Malek, J ;
Koga, N .
JOURNAL OF PHYSICAL CHEMISTRY A, 2000, 104 (46) :10777-10782
[10]   The Role of A-Site Ion Nonstoichiometry in the Oxygen Absorption Properties of Sr1+xCo0.8Fe0.2O3 Oxides [J].
He, Yufeng ;
Zhu, Xuefeng ;
Yang, Weishen .
AICHE JOURNAL, 2011, 57 (01) :87-95