Atmospheric plasma sprayed thick thermal barrier coatings with high segmentation crack density

被引:257
作者
Guo, HB [1 ]
Vassen, R [1 ]
Stöver, D [1 ]
机构
[1] Forschungszentrum Julich, Inst Werkstoffe & Verfahren Energietech 1, D-52425 Julich, Germany
关键词
thermal barrier coatings; segmentation crack density; substrate temperature; passage thickness; thermal shock;
D O I
10.1016/j.surfcoat.2004.01.002
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Atmospheric plasma sprayed thick thermal barrier coatings (TBCs), comprising of 1.5 mm thickness yttria stabilized zirconia (YSZ) coating, have been developed for increasing thermal protection of combustor applications. Different segmentation crack densities of the YSZ coating were created by controlling the deposition conditions. It was found that the substrate temperature played a dominant role in determining the segmentation crack density. The density was found to increase with the increase of substrate temperature and liquid splat temperature. High passage thickness, if achieved by low plasma gun speed, contributed to improve the segmentation crack density. The density could not be effectively improved by increasing the powder feed rate, although a high passage thickness was obtained in this case. The pores, mainly consisting of delaminations with the radii range between 0.02 and 1 mum, prevent the segmentation cracks from propagation. The coatings sprayed at high substrate temperature show an excellent intersplat bonding and often even continuous columnar grains through several splats. Additionally, horizontally branching cracks were also formed together with the segmentation cracks when a high lamellar thickness was used during the spraying. Thermal cycling tests showed that the coating with a segmentation crack density of approximately 3.6 mm(-1) had a lifetime of more than 1700 cycles at 1238degreesC (surface)/938degreesC (bond coat), indicative of excellent thermal shock resistance. Failure of the TBCs occurred by chipping in the surface layer of YSZ coating, which is different from the traditional interface delamination failure occurred with thinner TBCs. (C) 2004 Elsevier B.V All rights reserved.
引用
收藏
页码:353 / 363
页数:11
相关论文
共 40 条
[1]   Improved sealing treatments for thick thermal barrier coatings [J].
Ahmaniemi, S ;
Vuoristo, P ;
Mäntylä, T .
SURFACE & COATINGS TECHNOLOGY, 2002, 151 :412-417
[2]   Sealing procedures for thick thermal barrier coatings [J].
Ahmaniemi, S ;
Tuominen, J ;
Vuoristo, P ;
Mäntylä, T .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2002, 11 (03) :320-332
[3]   CHARACTERIZATION OF MICROSTRUCTURAL DEFECTS IN PLASMA-SPRAYED THERMAL BARRIER COATINGS [J].
BENGTSSON, P ;
JOHANNESSON, T .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 1995, 4 (03) :245-251
[4]  
BENGTSSON P, 1999, GAS TURBINE MAT TECH, P92
[5]  
BRINK RC, 1989, J ENG GAS TURB POWER, V111, P570
[6]  
CTIBOR P, 2001, NEW SURFACES NEW MIL, P677
[7]   MECHANISMS OF DEGRADATION AND FAILURE IN A PLASMA-DEPOSITED THERMAL BARRIER COATING [J].
DEMASIMARCIN, JT ;
SHEFFLER, KD ;
BOSE, S .
JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1990, 112 (04) :521-526
[8]  
FERRIERE A, 1994, J THERM SPRAY TECHN, V3, P362
[9]  
FUNKE C, 1997, UNITED FORUM SCI TEC, P277
[10]   Functionally graded ZrO2-NiCrAlY, coatings prepared by plasma spraying using pre-mixed, spheroidized powders [J].
Gu, YW ;
Khor, KA ;
Fu, YQ ;
Wang, Y .
SURFACE & COATINGS TECHNOLOGY, 1997, 96 (2-3) :305-312