Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments

被引:290
作者
Ehlers, J.
Young, D. J.
Smaardijk, E. J.
Tyagi, A. K.
Penkalla, H. J.
Singheiser, L.
Quadakkers, W. J. [1 ]
机构
[1] Forschungszentrum Julich, Inst Mat & Proc Energy Syst, D-52425 Julich, Germany
[2] Univ New S Wales, Sydney, NSW, Australia
[3] Indira Gandhi Ctr Atom Res, Kalpakkam 603102, Tamil Nadu, India
关键词
steel; SIMS; TEM; selective oxidation; kinetic parameters;
D O I
10.1016/j.corsci.2006.02.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The short term (similar to 100 h) oxidation behaviour of the 9%Cr steel P91 was studied at 650 degrees C in N-2-O-2-H2O gas mixtures containing a relatively low oxygen level of 1%. The oxidation kinetics were measured thermogravimetrically and the oxide scale growth mechanisms were studied using (H2O)-O-18-tracer with subsequent analyses of oxide scale composition and tracer distribution by MCs+-SIMS depth profiling. The corrosion products were additionally characterised by light optical microscopy, SEM-EDX and XRD. It was found that the transition from protective, Cr-rich oxide formation into non-protective mixed oxide scales is governed by the ratio H2O(g)/O-2 ratio rather than the absolute level of H2O(g). The results of the tracer studies in combination with the data obtained from experiments involving in situ gas changes clearly illustrated that under the prevailing conditions the penetration of water vapour molecules triggers the enhanced oxidation and sustains the high growth rates of the poorly protective Fe-rich oxide scale formed in atmospheres with high H2O(g)/O-2 ratios. The experimental observations can be explained if one assumes the scale growth to be governed by a competitive adsorption of oxygen and water vapour molecules on external and internal surfaces of the oxide scales in combination with the formation of a volatile Fe-hydroxide during transient oxidation. The formation of the non-protective Fe-rich oxide scales is suppressed in atmospheres with low H2O(g)/O-2-ratios, and the healing of any such scale is promoted. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3428 / 3454
页数:27
相关论文
共 39 条
[1]   Steam oxidation of slurry aluminide coatings on ferritic steels for advanced coal-fired steam power plants [J].
Agüero, A ;
Muelas, R .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 :957-964
[2]   The influence of water vapor on the corrosion of chromia-forming steels [J].
Asteman, H ;
Segerdahl, K ;
Svensson, JE ;
Johansson, LG .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 5, PTS 1 AND 2, 2001, 369-3 :277-285
[3]   Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor [J].
Asteman, H ;
Svensson, JE ;
Johansson, LG ;
Norell, M .
OXIDATION OF METALS, 1999, 52 (1-2) :95-111
[4]  
Birks N., 1983, INTRO HIGH TEMPERATU
[5]  
BOWEN AW, 1970, METALL TRANS, V1, P2767
[6]   International workshop on high-temperature corrosion [J].
Douglass, DL ;
Kofstad, P ;
Rahmel, A ;
Wood, GC .
OXIDATION OF METALS, 1996, 45 (5-6) :529-620
[8]  
EHLERS J, 2001, JUL3883 FRG
[9]  
Ehlers RJ, 2001, EUR FED CORR PUBL, P178
[10]  
Ennis P. J., 2001, ADV MAT TECHNOLOGY F, P187