Mesopore size dependence of the ionic diffusivity in alumina based composite lithium ionic conductors

被引:46
作者
Maekawa, Hideki [1 ]
Fujimaki, Yutaka
Shen, Hangyan
Kawamura, Junichi
Yamamura, Tsutomu
机构
[1] Tohoku Univ, Grad Sch Engn, Sendai, Miyagi 9808579, Japan
[2] PRESTO, Japan Sci & Technol Corp, Kawaguchi 3320012, Japan
[3] Tohoku Univ, Interdisciplinary Res Ctr, Sendai, Miyagi 9808578, Japan
[4] Tohoku Univ, Inst Multidisciplinary Res, Sendai, Miyagi 9808577, Japan
关键词
mesoporous alumina; lithium iodide; composite ionic conductor; pore size dependence;
D O I
10.1016/j.ssi.2006.02.002
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ordered-mesoporous Al2O3 was synthesized by a sol-gel method using neutral copolymer surfactants as structure-directing agents. The pore size was controlled over the 3-15nm range by the use of various surfactants. Composites composed of the synthesized mesoporous Al2O3 and a lithium ion conductor (LiI) were prepared. The maximum dc electrical conductivity, 2.6 x 10(-4) S cm(-1) at 298K, was observed for 50 LiI.50 Al2O3 composite with 4.2nm average mesopore size, which was considerably higher than the previously reported LiI-alumina composites. A systematic dependence of conductivity upon pore size was observed, in which conductivity increased with decreasing pore size, except for samples with a pore size of 2.8nm. The lithium ion diffusion coefficient determined by the Li-7 pulsed field gradient nuclear magnetic resonance (PFG-NMR) showed excellent agreement with the measured conductivity calculated by the Nemst-Einstein equation. On the other hand, lithium migration activation energies obtained by quasielastic neutron scattering (QENS) and Li-7 NMR spin-lattice relaxation time (T-1) were considerably smaller than those obtained from electrical conductivity and PFG-NMR. This could be explained by the ion migration mechanism in heterogeneous composites and a possible enhancement of conductivity in mesoscopically confined spaces. (c) 2006 Published by Elsevier B.V.
引用
收藏
页码:2711 / 2714
页数:4
相关论文
共 11 条
[1]   CONDUCTION CHARACTERISTICS OF LITHIUM IODIDE ALUMINUM OXIDE SOLID ELECTROLYTES [J].
LIANG, CC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1973, 120 (10) :1289-1292
[2]   Size dependent ionic conductivity observed for ordered-mesoporous-alumina-ionic conductor composites [J].
Maekawa, H ;
Tanaka, R ;
Shen, HY ;
Fujimaki, Y ;
Yamamura, T ;
Shirata, K ;
Kawai, M .
SOLID STATE IONICS: THE SCIENCE AND TECHNOLOGY OF IONS IN MOTION, 2004, :851-857
[3]   Size-dependent ionic conductivity observed for ordered mesoporous alumina-LiI composite [J].
Maekawa, H ;
Tanaka, R ;
Sato, T ;
Fujimaki, Y ;
Yamamura, T .
SOLID STATE IONICS, 2004, 175 (1-4) :281-285
[4]   Meso/macroporous inorganic oxide monoliths from polymer foams [J].
Maekawa, H ;
Esquena, J ;
Bishop, S ;
Solans, C ;
Chmelka, BF .
ADVANCED MATERIALS, 2003, 15 (7-8) :591-596
[5]  
MAEKAWA H, 2003, MRS S P, V756
[7]   IONIC-CONDUCTION IN-SPACE CHARGE REGIONS [J].
MAIER, J .
PROGRESS IN SOLID STATE CHEMISTRY, 1995, 23 (03) :171-263
[8]   ELECTRICAL-CONDUCTIVITY OF THE LIL-H2O-AL2O3 SYSTEM [J].
PACK, S ;
OWENS, B ;
WAGNER, JB .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (10) :2177-2179
[9]   PROPERTIES OF LII - ALUMINA COMPOSITE ELECTROLYTES [J].
POULSEN, FW ;
ANDERSEN, NH ;
KINDL, B ;
SCHOONMAN, J .
SOLID STATE IONICS, 1983, 9-10 (DEC) :119-122
[10]   High proton conductivity of niesoporous Al2O3 [J].
Shen, HY ;
Maekawa, H ;
Fujimaki, Y ;
Kawada, K ;
Yamamura, T .
SOLID STATE IONICS: THE SCIENCE AND TECHNOLOGY OF IONS IN MOTION, 2004, :187-193