Densification of hybrid silica-titania sol-gel films studied by ellipsometry and FTIR

被引:76
作者
Seco, AM [1 ]
Gonçalves, MC [1 ]
Almeida, RM [1 ]
机构
[1] Univ Tecn Lisboa, INESC, Dept Engn Mat, Inst Super Tecn, P-1000 Lisbon, Portugal
来源
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY | 2000年 / 76卷 / 03期
关键词
silica-titania films; hybrid sol-gel films; ellipsometry; infrared absorption (FTIR) spectroscopy;
D O I
10.1016/S0921-5107(00)00442-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hybrid silica-titania films were prepared via soi-gel processing, by dip-coating on silicon wafer substrates, from organically-modified silane and titanium isopropoxide precursors. These hybrid sol-gel films were then subjected to selected heat treatments at temperatures up to 950 degrees C and their densification was Followed by ellipsometry and infrared absorption (FTIR) spectroscopy. The volume fraction of residual porosity was estimated, based on the refractive index data. A clear correlation was observed between the intensity of the infrared spectral shoulder near 1150 cm(-1) and the porosity values, for the different heat treatment temperatures. For any treatment up to 950 degrees C, the porosity of the hybrid silica-titania gel films was higher than that of the corresponding inorganic gel films, while both continuously decreased with increasing heat treatment temperature. The residual Si-CH3 groups, whose presence was identified in the hybrid silica-titania films until a temperature near 500 degrees C, tend to be transformed into Si-OH (silanol) groups as they are eliminated. Most silanol groups are eliminated at a temperature near 600 degrees C. The hybrid silica-titania films were found to have a more porous and more compliant gel network than the corresponding inorganic films, while their structure appears to exhibit a smaller spread in the Si-O-Si intertetrahedral angle distribution. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
引用
收藏
页码:193 / 199
页数:7
相关论文
共 24 条
[1]   XPS and NEXAFS studies of rare-earth doped amorphous sol-gel films [J].
Almeida, RM ;
Vasconcelos, HC ;
Goncalves, MC ;
Santos, LF .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1998, 232 :65-71
[2]   Optical loss mechanisms in nanocomposite sol-gel planar waveguides [J].
Almeida, RM ;
Morais, PJ ;
Vasconcelos, HC .
SOL-GEL OPTICS IV, 1997, 3136 :296-303
[3]  
ALMEIDA RM, 1994, PROC SPIE, V2288, P678, DOI 10.1117/12.189004
[4]   EXAFS and XANES studies of silica-titania sol-gel films [J].
Almeida, RM ;
Marques, MID ;
Orignac, X .
JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 1997, 8 (1-3) :293-297
[5]   Er3+-doped multicomponent silicate glass planar waveguides prepared by sol-gel processing [J].
Almeida, RM ;
Du, XM ;
Barbier, D ;
Orignac, X .
JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 1999, 14 (02) :209-216
[6]   CHARACTERIZATION OF SILICA-GELS BY INFRARED REFLECTION SPECTROSCOPY [J].
ALMEIDA, RM ;
GUITON, TA ;
PANTANO, CG .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1990, 121 (1-3) :193-197
[7]   STRUCTURAL INVESTIGATION OF SILICA-GEL FILMS BY INFRARED-SPECTROSCOPY [J].
ALMEIDA, RM ;
PANTANO, CG .
JOURNAL OF APPLIED PHYSICS, 1990, 68 (08) :4225-4232
[8]   Spectroscopy and structure of sol-gel systems [J].
Almeida, RM .
JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 1998, 13 (1-3) :51-59
[9]  
ALMEIDA RM, 1997, P SPIE CR, V68, P172
[10]   Microstructural and optical properties of sol-gel silica-titania waveguides [J].
Brusatin, G ;
Guglielmi, M ;
Innocenzi, P ;
Martucci, A ;
Battaglin, C ;
Pelli, S ;
Righini, G .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1997, 220 (2-3) :202-209