Use of fluoroalkylsilanes as non-stick coatings for thermal by-products of linoleic acid

被引:15
作者
Mostefai, M
Auriac, Y
Shanahan, MER
Bressan, J
Meslif, A
机构
[1] Univ Evry Val Essonne, Ecole Natl Super Mines, Ctr Mat PM Fourt, F-91003 Evry, France
[2] Gaz France, Direct Rech, F-93211 St Denis La Plaine, France
关键词
destructive testing; linoleic acid; fluoroalkylsilanes; non-stick;
D O I
10.1016/S0143-7496(99)00057-3
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The adhesion of linoleic acid heated at different temperatures ranging from 220 to 280 degrees C on three different substrates has been investigated. During heating, several chemical modifications of linoleic acid occur and strong adhesion to the substrate develops. In order to obtain quantitative data, a specific adhesion test has been developed. The adhesion of linoleic acid at high temperature can be strongly reduced by using fluoroalkylsilane-treated plates. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:257 / 261
页数:5
相关论文
共 8 条
[1]  
ALBINSON RB, 1990, Patent No. 367438
[2]  
Arkles B., 1992, SILANES OTHER COUPLI, P91
[3]   DETERMINATION OF AMINO AND SILANOL FUNCTIONAL-GROUPS ON GLASS VIA CHEMICAL DERIVATIZATION AND ESCA [J].
DANG, TA ;
GNANASEKARAN, R .
SURFACE AND INTERFACE ANALYSIS, 1990, 15 (02) :113-118
[4]   FRICTION AND WEAR OF SELF-ASSEMBLED TRICHLOROSILANE MONOLAYER FILMS ON SILICON [J].
DEPALMA, V ;
TILLMAN, N .
LANGMUIR, 1989, 5 (03) :868-872
[5]  
KAZUFUMI O, 1992, Patent No. 571896
[6]  
KAZUFUMI O, 1992, Patent No. 493747
[7]   Fluoroalkylsilanes as non-stick coatings: adhesion of glucose and its thermal byproducts [J].
Mostefai, M ;
Auriac, Y ;
Shanahan, MER ;
Bressan, J ;
Meslif, A .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1998, 18 (04) :273-281
[8]   ADDITIVE AND NONADDITIVE SURFACE-TENSION COMPONENTS AND THE INTERPRETATION OF CONTACT ANGLES [J].
VANOSS, CJ ;
GOOD, RJ ;
CHAUDHURY, MK .
LANGMUIR, 1988, 4 (04) :884-891