Investigating the correlation between nano-impact fracture resistance and hardness/modulus ratio from nanoindentation at 25-500 °C and the fracture resistance and lifetime of cutting tools with Ti1-xAlxN (x=0.5 and 0.67) PVD coatings in milling operations

被引:91
作者
Beake, B. D.
Smith, J. F.
Gray, A.
Fox-Rabinovich, G. S.
Veldhuis, S. C.
Endrino, J. L.
机构
[1] Micro Mat Ltd, Wrexham, Wales
[2] McMaster Univ, Dept Mech Engn, Hamilton, ON L8S 4L7, Canada
关键词
TiAlN; AlTiN coatings; nano-impact fracture resistance; cutting tool life;
D O I
10.1016/j.surfcoat.2006.09.118
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A novel laboratory technique, nano-impact testing, has been used to test Ti1-xAlxN (x=0.5 and 0.67) PVD coated WC-Co inserts at 25-500 degrees C . Cutting tool life was studied under conditions of face milling of the structural AISI 1040 steel; the end milling of hardened 4340 steel (HRC 40) and TiAl6V4 alloy A correlation was found between the results of the rapid nano-impact test and milling tests. When x=0.67 improved resistance to fracture was found during milling operations and also in the nano-impact test of this coating compared to when x=0.50. The coating protects the cutting tool surface against the chipping that is typical for cutting operations with intensive adhesive interaction with workpiece materials such as machining of Ti-based alloys. The results give encouragement that the elevated temperature nano-impact test can be used to predict the wear and fracture resistance of hard coatings during milling operations. At 500 degrees C nanoindentation shows there is a lower HIE, ratio for the PVD coatings compared to room temperature, consistent with reduced fracture observed at this temperature in the nano-impact test. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:4585 / 4593
页数:9
相关论文
共 23 条
[1]   Evaluation of the fracture resistance of DLC coatings on tool steel under dynamic loading [J].
Beake, BD .
SURFACE & COATINGS TECHNOLOGY, 2005, 198 (1-3) :90-93
[2]   Nano-impact testing-an effective tool for assessing the resistance of advanced wear-resistant coatings to fatigue failure and delamination [J].
Beake, BD ;
Smith, JF .
SURFACE & COATINGS TECHNOLOGY, 2004, 188 :594-598
[3]   Evaluating the fracture properties and fatigue wear of tetrahedral amorphous carbon films on silicon by nano-impact testing [J].
Beake, BD ;
Lau, SR ;
Smith, JF .
SURFACE & COATINGS TECHNOLOGY, 2004, 177 :611-615
[4]   Micro-impact testing: A new technique for investigating thin film toughness, adhesion, erosive wear resistance, and dynamic hardness [J].
Beake, BD ;
Goodes, SR ;
Smith, JF .
SURFACE ENGINEERING, 2001, 17 (03) :187-192
[5]   High-temperature nanoindentation testing of fused silica and other materials [J].
Beake, BD ;
Smith, JF .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 2002, 82 (10) :2179-2186
[6]   Scaling, dimensional analysis, and indentation measurements [J].
Cheng, YT ;
Cheng, CM .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2004, 44 (4-5) :91-149
[7]  
Fox-Rabinovich G., 2006, SELF ORG FRICTION AD, P121
[8]   Effect of mechanical properties measured at room and elevated temperatures on the wear resistance of cutting tools with TiAlN and AlCrN coatings [J].
Fox-Rabinovich, GS ;
Beake, BD ;
Endrino, JL ;
Veldhuis, SC ;
Parkinson, R ;
Shuster, LS ;
Migranov, MS .
SURFACE & COATINGS TECHNOLOGY, 2006, 200 (20-21) :5738-5742
[9]   Elastic and plastic work of indentation as a characteristic of wear behavior for cutting tools with nitride PVD coatings [J].
Fox-Rabinovich, GS ;
Veldhuis, SC ;
Scvortsov, VN ;
Shuster, LS ;
Dosbaeva, GK ;
Migranov, MS .
THIN SOLID FILMS, 2004, 469 :505-512
[10]  
FOXRABINOVICH GS, IN P RESS SURF COAT, DOI DOI 10.1016/J.SURFCOAT.2006.08.075