Hydrolytic and enzymatic degradation of copoly(ester amide)s based on L-tartaric and succinic acids

被引:16
作者
Alla, A [1 ]
Rodríguez-Galán, A [1 ]
Muñoz-Guerra, S [1 ]
机构
[1] Univ Politecn Cataluna, ETSEIB, Dept Engn Quim, Diagonal 647, E-08028 Barcelona, Spain
关键词
poly(ester amide)s; copoly(ester amide)s hydrolytic degradation; enzymatic degradation;
D O I
10.1016/S0032-3861(00)00070-7
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The hydrolytic and enzymatic degradation of a series of crystalline copoly(ester amide)s derived from L-tartaric and succinic acids, 1,6 hexanediamine and 1,6-hexanediol with ester/amide groups ratios 3/97, 10/90, 15/85 and 20/80 was investigated. The hydrolytic degradation study was carried out at 37 degrees C in buffered solution at pH 7.4. Changes taking place in sample weight, molecular weight, chemical constitution and thermal properties of the polymer were evaluated. Degradation proceeded with a notable increment in crystallinity and entailing slight but significant changes in the T-g and T-m temperatures. It was found that copoly(ester amide)s degraded faster than the parent poly(hexamethylene-di-O-methyl-L-tartaramide) and that the race of degradation increased with the content in ester groups. It was also showed that degradation is accompanied by formation of cyclic succinimide units indicative of a scission mechanism based on the occurrence of intramolecular imidation reactions. The enzymatic degradation of these copoly(ester amide)s with papain was comparatively examined for a preliminary evaluation of their potential biodegradability. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:6995 / 7002
页数:8
相关论文
共 22 条
[1]   Degradable poly(ester amide)s based on L-tartaric acid [J].
Alla, A ;
RodriguezGalan, A ;
deIlarduya, AM ;
MunozGuerra, S .
POLYMER, 1997, 38 (19) :4935-4944
[2]   SYNTHESIS AND STUDY OF NOVEL BIODEGRADABLE OLIGO(ESTER AMIDE)S BASED ON SEBACIC ACID, OCTADECANEDIOIC ACID, 1,6-HEXANEDIAMINE AND EPSILON-CAPROLACTONE .2. [J].
ARVANITOYANNIS, I ;
NAKAYAMA, A ;
KAWASAKI, N ;
YAMAMOTO, N .
POLYMER, 1995, 36 (04) :857-866
[3]   COPOLYMERIZATION AND DEGRADATION OF POLY(LACTIC ACID CO-LYSINE) [J].
BARRERA, DA ;
ZYLSTRA, E ;
LANSBURY, PT ;
LANGER, R .
MACROMOLECULES, 1995, 28 (02) :425-432
[4]   OPTICALLY-ACTIVE POLYAMIDES DERIVED FROM L-TARTARIC ACID [J].
BOU, JJ ;
RODRIGUEZGALAN, A ;
MUNOZGUERRA, S .
MACROMOLECULES, 1993, 26 (21) :5664-5670
[5]   SYNTHESIS OF STEREOREGULAR POLYGLUCONAMIDES FROM D-GLUCOSE AND D-GLUCOSAMINE [J].
BUENO, M ;
GALBIS, JA ;
GARCIAMARTIN, MG ;
DEPAZ, MV ;
ZAMORA, F ;
MUNOZGUERRA, S .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1995, 33 (02) :299-305
[6]  
BuenoMartinez M., 1997, MACROMOLECULES, V30, P3197
[7]   SYNTHESIS AND PHYSICO-MECHANICAL PROPERTIES OF ALIPHATIC POLYESTERAMIDES [J].
CASTALDO, L ;
DECANDIA, F ;
MAGLIO, G ;
PALUMBO, R ;
STRAZZA, G .
JOURNAL OF APPLIED POLYMER SCIENCE, 1982, 27 (05) :1809-1822
[8]   SYNTHESIS, CHARACTERIZATION, AND DEGRADATION OF BLOCK POLYESTERAMIDES CONTAINING POLY(L-LACTIDE) SEGMENTS [J].
DESIMONE, V ;
MAGLIO, G ;
PALUMBO, R ;
SCARDI, V .
JOURNAL OF APPLIED POLYMER SCIENCE, 1992, 46 (10) :1813-1820
[9]   SEGMENTED COPOLYMERS WITH POLY(ESTER AMIDE) UNITS OF UNIFORM LENGTH - SYNTHESIS [J].
GAYMANS, RJ ;
DEHAAN, JL .
POLYMER, 1993, 34 (20) :4360-4364
[10]   DEGRADATION OF NONALTERNATING POLY(ESTER-AMIDES) [J].
GONSALVES, KE ;
CHEN, X ;
CAMERON, JA .
MACROMOLECULES, 1992, 25 (12) :3309-3312