Systematic assessment and validation of compliance-based crack closure measurements in fatigue

被引:45
作者
Xu, YG [1 ]
Gregson, PJ [1 ]
Sinclair, I [1 ]
机构
[1] Univ Southampton, Sch Engn Sci, Mat Res Grp, Highfield SO17 1BJ, England
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2000年 / 284卷 / 1-2期
关键词
Al alloy; fatigue; crack growth; closure measurements; shielding;
D O I
10.1016/S0921-5093(00)00758-9
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Different methods of closure measurement and issues related to the identification of closure points are examined. Based on compliance curves obtained from crack mouth clip gauges and near-tip strain gauges, a systematic assessment of closure measurements has been made by a variety of non-subjective methods. Closure results obtained from compliance curves are also compared with direct crack tip observations. For results obtained on a commercial Al alloy, AA2024-T351 plate, it is shown that curve fitting methods based on a combination of linear and quadratic functions provide particularly sensitive and consistent closure measurements. The potential separation of plane stress and plane strain closure effects that arise in real, three-dimensional specimens is demonstrated via a combination of global compliance measurements and the use of side-grooved specimens. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:114 / 125
页数:12
相关论文
共 29 条
[1]  
Allison J.E., 1988, ASTM STP, P171
[2]  
ASTM, 1995, E64795 ASTM, P578
[3]  
BACHMANN V, 1976, J TEST EVAL, V4, P257, DOI 10.1520/JTE10210J
[4]   FATIGUE CRACK CLOSURE [J].
DAVIDSON, DL .
ENGINEERING FRACTURE MECHANICS, 1991, 38 (06) :393-402
[5]   FATIGUE CRACK-GROWTH THROUGH ARALL-4 AT AMBIENT-TEMPERATURE [J].
DAVIDSON, DL ;
AUSTIN, LK .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1991, 14 (10) :939-951
[6]  
DEKONING AU, 1982, TR81141 L NLR
[7]  
Elber W., 1971, AMAGE TOLERANCE AIRC, P230, DOI DOI 10.1520/STP486-EB
[8]  
FELLOWS LJ, 1997, ADV FRACTURE RES, P2552
[9]   CRACK CLOSURE - IS IT JUST A SURFACE PHENOMENON [J].
FLECK, NA ;
SMITH, RA .
INTERNATIONAL JOURNAL OF FATIGUE, 1982, 4 (03) :157-160
[10]   Direct observation of crack opening as a function of applied load in the interior of a notched tensile sample of Al-Li 2090 [J].
Guvenilir, A ;
Breunig, TM ;
Kinney, JH ;
Stock, SR .
ACTA MATERIALIA, 1997, 45 (05) :1977-1987