摘要
The chemical composition, microstructure and mechanical properties of Tyranno Lox-E fibre were studied in the as-received state and after annealing in inert atmosphere. The fibre consists of SiC nanocrystals of 2-3 nm, free carbon aggregates of 4-5 distorted aromatic layers and 1-3 nm in length and an amorphous silicon (titanium) oxycarbide phase. Except for evolution of residual hydrogen and a slight densification, the fibre is chemically and structurally stable and retains a high strength up to 1300 degrees C. Beyond 1300 degrees C, superficial degradation resulting from decomposition of the oxycarbide into SiO((g)) and CO((g)) induces a decrease of strength. Compared with bulk polycrystalline SiC, the fibre has a low creep resistance at high temperature, mainly because of the nanometric size of the SiC crystals but also because of the presence at the grain boundary of the oxycarbide phase (viscous and chemically unstable) and of the poorly organized free carbon phase (chemically and structurally unstable). (C) 1998 Chapman & Hall.
引用
收藏
页码:901 / 911
页数:11
相关论文
共 38 条
[1]   EFFECT OF THERMOCHEMICAL TREATMENTS ON THE STRENGTH AND MICROSTRUCTURE OF SIC FIBERS [J].
BENDER, BA ;
WALLACE, JS ;
SCHRODT, DJ .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (04) :970-976
[2]   TENSILE CREEP-BEHAVIOR OF A SILICON CARBIDE-BASED FIBER WITH A LOW-OXYGEN CONTENT [J].
BODET, R ;
BOURRAT, X ;
LAMON, J ;
NASLAIN, R .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (03) :661-677
[3]  
Bodet R, 1996, J AM CERAM SOC, V79, P2673, DOI 10.1111/j.1151-2916.1996.tb09033.x
[4]   COMPOSITION MICROSTRUCTURE PROPERTY RELATIONSHIPS IN CERAMIC MONOFILAMENTS RESULTING FROM THE PYROLYSIS OF A POLYCARBOSILANE PRECURSOR AT 800 TO 1400-DEGREES-C [J].
BOUILLON, E ;
MOCAER, D ;
VILLENEUVE, JF ;
PAILLER, R ;
NASLAIN, R ;
MONTHIOUX, M ;
OBERLIN, A ;
GUIMON, C ;
PFISTER, G .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (06) :1517-1530
[5]   NON-METAL-METAL TRANSITION IN A NON-CRYSTALLINE CARBON [J].
CARMONA, F ;
DELHAES, P ;
KERYER, G ;
MANCEAU, JP .
SOLID STATE COMMUNICATIONS, 1974, 14 (11) :1183-1187
[6]  
CHALLON G, 1997, J MATER SCI, V32, P327
[7]   ELECTRONIC-PROPERTIES OF DISORDERED SIC MATERIALS [J].
CHAUVET, O ;
ZUPPIROLI, L ;
SOLOMON, I .
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1992, 11 (1-4) :303-306
[8]   Correlation between microstructure and mechanical behaviour at high temperatures of a SiC fibre with a low oxygen content (Hi-Nicalon) [J].
Chollon, G ;
Pailler, R ;
Naslain, R ;
Olry, P .
JOURNAL OF MATERIALS SCIENCE, 1997, 32 (05) :1133-1147
[9]  
CLARK TJ, 1986, CERAM ENG SCI P, V7, P901
[10]  
CLARK TJ, 1985, CERAM ENG SCI P, V6, P576