Crystal chemistry and ion conductivity of the Na1+xTi2-xAlx(PO4)3 (0 ≤ x ≤ 0.9) NASICON series

被引:49
作者
Mouahid, FE
Bettach, M
Zahir, M
Maldonado-Manso, P
Bruque, S [1 ]
Losilla, ER
Aranda, MAG
机构
[1] Univ Malaga, Dept Quim Inorgan Cristalog & Mineral, E-29071 Malaga, Spain
[2] Univ Chouaib Doukkali, Fac Sci, Dept Chim, LPCM, El Jadida, Morocco
关键词
D O I
10.1039/b004837m
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The Na1 + xTi2 - xAlx(PO4)(3) (0.0 less than or equal to x less than or equal to 0.9) solid solution has been prepared as a polycrystalline powder. These compounds crystallise in the NASICON type structure, R (3) over barc space group, and the crystal structures have been characterised by the Rietveld method with laboratory powder diffraction data. The Ti/Al atoms are randomly distributed over the octahedral site of the NASICON framework. The negatively charged framework is neutralised by the Na+ cations which are distributed over the M1 site, fully occupied, and M2 site, partly occupied. The cell parameter evolution along the series agrees with the substitution of larger Ti4+ by smaller Al3+ cations. The thermal expansion coefficients were determined from a thermodiffractometric study of Na1.8Ti1.2Al0.8(PO4)(3). The ion conductivity of the samples rises as the charge carrier number (x) increases. The activation energies deduced from the Arrhenius plots are close to 0.50 eV. The overall conductivities are near to 10(-5) S cm(-1) at 200 degreesC.
引用
收藏
页码:2748 / 2753
页数:6
相关论文
共 22 条
[1]  
[Anonymous], 1994, LAUR86748 LOS AL NAT
[2]   IONIC-CONDUCTIVITY OF THE LITHIUM TITANIUM PHOSPHATE (LI1+XALXTI2-X(PO4)3), (LI1+XSCXTI2-X(PO4)3), (LI1+XYXTI2-X(PO4)3), (LI1+XLAXTI2-X(PO4)3 SYSTEMS [J].
AONO, H ;
SUGIMOTO, E ;
SADAOKA, Y ;
IMANAKA, N ;
ADACHI, GY .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1989, 136 (02) :590-591
[3]   ELECTRICAL-PROPERTIES OF SINTERED LITHIUM TITANIUM PHOSPHATE CERAMICS (LI1+XMXTI2-X(PO4)3, M-3+ = AL-3+, SC-3+, OR Y-3+) [J].
AONO, H ;
SUGIMOTO, E ;
SADAOKA, Y ;
IMANAKA, N ;
ADACHI, G .
CHEMISTRY LETTERS, 1990, (10) :1825-1828
[4]   ELECTRICAL-PROPERTIES AND CRYSTAL-STRUCTURE OF SOLID-ELECTROLYTE BASED ON LITHIUM HAFNIUM PHOSPHATE LIHF2(PO4)3 [J].
AONO, H ;
SUGIMOTO, E ;
SADAOKA, Y ;
IMANAKA, N ;
ADACHI, GY .
SOLID STATE IONICS, 1993, 62 (3-4) :309-316
[5]   IONIC-CONDUCTIVITY OF SOLID ELECTROLYTES BASED ON LITHIUM TITANIUM PHOSPHATE [J].
AONO, H ;
SUGIMOTO, E ;
SADAOKA, Y ;
IMANAKA, N ;
ADACHI, G .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1990, 137 (04) :1023-1027
[6]   ELECTRICAL-PROPERTIES AND SINTERABILITY FOR LITHIUM GERMANIUM PHOSPHATE LI1+XMXGE2-X(PO4)3, M=AL, CR, GA, FE, SC, AND IN SYSTEMS [J].
AONO, H ;
SUGIMOTO, E ;
SADAOKA, Y ;
IMANAKA, N ;
ADACHI, GY .
BULLETIN OF THE CHEMICAL SOCIETY OF JAPAN, 1992, 65 (08) :2200-2204
[7]   THE NASICON-TYPE TITANIUM PHOSPHATES LITI2(PO4)3, NATI2(PO4)3 AS ELECTRODE MATERIALS [J].
DELMAS, C ;
NADIRI, A ;
SOUBEYROUX, JL .
SOLID STATE IONICS, 1988, 28 :419-423
[8]   FAST NA+-ION TRANSPORT IN SKELETON STRUCTURES [J].
GOODENOUGH, JB ;
HONG, HYP ;
KAFALAS, JA .
MATERIALS RESEARCH BULLETIN, 1976, 11 (02) :203-220
[9]  
HAMEDOUNE S, 1986, MAT RES B, V21, P237
[10]   CRYSTAL-STRUCTURES AND CRYSTAL-CHEMISTRY IN SYSTEM NA1+XZR2SIXP3-XO12 [J].
HONG, HYP .
MATERIALS RESEARCH BULLETIN, 1976, 11 (02) :173-182