摘要
Environmental embrittlement types of six iron aluminides have been systematically evaluated using electrochemical hydrogen permeation measurement, hydrogen microprint technique and tensile test in this study. The results of hydrogen permeation and microprint technique show that three alpha - disordered solid solution structure of binary and ternary iron aluminides (Fe-10Al, Fe-18Al, and Fe-18Al-5Cr) have higher effective diffusivity and permeation rate than B2 ordered structure of binary and ternary iron aluminides (Fe-28Al, Fe-28Al-5Cr, and Fe-40Al). The tensile test of six iron aluminides in air, vacuum treatment and hydrogen precharged were analyzed and concluded. Three alpha - disordered solid solution structure of iron aluminides suffer in hydrogen environment which are quite different embrittlement mechanisms from those B2 ordered structure of iron aluminides with serious tensile loss in air by moisture induced embrittlement. (C) 2000 Kluwer Academic Publishers.
引用
收藏
页码:4121 / 4127
页数:7
相关论文
共 24 条
[1]  
BAHADUR A, 1991, J MATER SCI, V26, P2685, DOI 10.1007/BF02387737
[2]   Hydrogen diffusivity in iron aluminides determined by subscale microhardness profiling [J].
Banerjee, P ;
Balasubramaniam, R .
SCRIPTA MATERIALIA, 1998, 39 (09) :1215-1219
[3]   Mechanical behavior of chromium and titanium alloyed iron aluminides with mischmetal addition [J].
Banerjee, P ;
Balasubramaniam, R .
SCRIPTA MATERIALIA, 1998, 38 (07) :1143-1147
[4]  
CHENG XY, 1998, SCRIPTA MATER, V38, P1215
[5]  
CRANK J, 1977, MATH DIFFUSION, P44
[6]   1ST PRINCIPLES INVESTIGATION OF HYDROGEN EMBRITTLEMENT IN FEAL [J].
FU, CL ;
PAINTER, GS .
JOURNAL OF MATERIALS RESEARCH, 1991, 6 (04) :719-723
[7]   The effect of hydrogen on the hardness of Fe-Al alloys [J].
Hosoda, H ;
Mizuuchi, K ;
Inoue, K .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1997, 49 (08) :56-59
[8]   Fracture properties at ambient temperatures of iron aluminides fabricated by reactive hot-pressing [J].
Inoue, M ;
Suganuma, K ;
Niihara, K .
SCRIPTA MATERIALIA, 1998, 39 (10) :1477-1482
[9]   Effect of Zr and C additions on environmental embrittlement of Fe-28Al-5Cr aluminide [J].
Liu, CT ;
Wright, JL ;
Stoloff, NS .
SCRIPTA MATERIALIA, 1998, 38 (10) :1601-1606
[10]   The influence of microstructure on hydrogen transport in carbon steels [J].
Luu, WC ;
Wu, JK .
CORROSION SCIENCE, 1996, 38 (02) :239-245