Improved oxidation resistance of Ti with a thermal sprayed Ti3Al(O)-Al2O3 composite coating

被引:22
作者
Li, ZW
Gao, W
Ying, DY
Zhang, DL
机构
[1] Univ Auckland, Dept Chem & Mat Engn, Auckland, New Zealand
[2] Univ Waikato, Dept Mat & Proc Engn, Hamilton, New Zealand
关键词
titanium; intermetallic; composite; coating; oxidation;
D O I
10.1016/S1359-6462(03)00133-7
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A Ti3Al(O)-Al2O3 in situ composite was explored as a coating system for Ti using thermal spray. Oxidation tests at 700-800 degreesC showed that this coating remarkably decreased the oxidation rate and increased the scale spallation resistance compared with Ti. The mechanisms for these improvements were then briefly discussed. (C) 2003 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1649 / 1653
页数:5
相关论文
共 11 条
[2]   SYNTHESIS, PROPERTIES AND APPLICATIONS OF TITANIUM ALUMINIDES [J].
FROES, FH ;
SURYANARAYANA, C ;
ELIEZER, D .
JOURNAL OF MATERIALS SCIENCE, 1992, 27 (19) :5113-5140
[3]   A new high-temperature, oxidation-resistant Ti-based material [J].
Gao, W ;
Li, Z ;
Zhang, D .
OXIDATION OF METALS, 2002, 57 (1-2) :99-114
[4]  
Kofstad P., 1988, Elsevier Appl. Sci., V24, DOI [10.1002/crat.2170240408, DOI 10.1002/CRAT.2170240408]
[5]  
Miracle D.B., 2000, COMPREHENSIVE COMPOS, V3, P741
[6]  
Sauthoff G, 1995, INTERMETALLICS
[7]   Intermetallic-matrix composites - A review [J].
WardClose, CM ;
Minor, R ;
Doorbar, PJ .
INTERMETALLICS, 1996, 4 (03) :217-229
[8]   Reaction kinetics and microstructural evolution during the heating of high energy ball milled Al-TiO2 and Al-V2O5 composite powders [J].
Zhang, DL ;
Ying, DY ;
Adam, G .
METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, 2002, 386-3 :287-292
[9]  
ZHANG DL, Patent No. 6264719
[10]  
ZHU RZ, 1995, HIGH TEMP CORROSION