Preparation of sulfonated ordered mesoporous carbon and its use for the esterification of fatty acids

被引:167
作者
Peng, Li [1 ]
Philippaerts, An [1 ]
Ke, Xiaoxing [2 ]
Van Noyen, Jasper [1 ]
De Clippel, Filip [1 ]
Van Tendeloo, Gustaaf [2 ]
Jacobs, Pierre A. [1 ]
Sels, Bert F. [1 ]
机构
[1] Katholieke Univ Leuven, Ctr Surface Chem & Catalysis, B-3001 Heverlee, Belgium
[2] Univ Antwerp, EMAT, B-2020 Antwerp, Belgium
关键词
Mesoporous carbon; Esterification; Acid catalysis; Sulfonation; SOLID ACID; ACTIVATED CARBON; GREEN CHEMISTRY; BIODIESEL PRODUCTION; SUGAR CATALYST; WATER; OXIDATION; SILICAS;
D O I
10.1016/j.cattod.2009.07.066
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Mesoporous carbon, which can be replicated from mesoporous silica and whose surface is hydrophobic, can be an ideal catalyst for the esterification of fatty acids. Here we report an easy and low cost way to prepare sulfonic acid group-functionalized mesoporous carbon. A sample of calcined mesoporous silica SBA-15 was added to an aqueous sucrose solution followed by drying and calcination at different temperatures. In contrast to existing procedures, the obtained hybrid Si/C material was then first sulfonated in H2SO4, before the final removal of the silica template in order to stabilize the porous structure towards the liquid phase sulfonation treatment. Thus the silica-carbon composites, instead of the mesoporous carbon, were successfully sulfonated to introduce -SO3H groups, while keeping the ordered mesoporous structure intact. The influence of carbonization temperature was investigated, suggesting an optimum temperature of 873 K. The SO3H group-functionalized mesoporous carbon, denoted as CMK-3-873-SO3H, was characterized by means of XRD, N-2 physisorption, SEM, FT-IR, elemental analysis and TEM. It followed that a uniform mesoporous carbon was obtained with an average pore size of 3.89 nm, a specific surface of 807 m(2)/g and a -SO3H group loading of 0.39 meq/g of dry material. Compared with other solid acid catalysts, the resulting material shows enhanced activity in the acid-catalyzed esterification of oleic acid with methanol, and can be used repeatedly. The increased catalytic performance is attributed to the hydrophobic surface and larger pore size of the new catalyst. It can effectively accommodate long chain fatty acids and reject formed water, making the active sites easily accessible. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:140 / 146
页数:7
相关论文
共 29 条
[1]   OXIDATION OF ACTIVATED CARBON IN LIQUID-PHASE - STUDY BY FT-IR [J].
ACEDORAMOS, M ;
GOMEZSERRANO, V ;
VALENZUELACALAHORRO, C ;
LOPEZPEINADO, AJ .
SPECTROSCOPY LETTERS, 1993, 26 (06) :1117-1137
[2]   Origins, current status, and future challenges of green chemistry [J].
Anastas, PT ;
Kirchhoff, MM .
ACCOUNTS OF CHEMICAL RESEARCH, 2002, 35 (09) :686-694
[3]   Surface oxides on carbon and their analysis: a critical assessment [J].
Boehm, HP .
CARBON, 2002, 40 (02) :145-149
[4]   Starbons: New starch-derived mesoporous carbonaceous materials with tunable properties [J].
Budarin, Vitaly ;
Clark, James H. ;
Hardy, Jeffrey J. E. ;
Luque, Rafael ;
Milkowski, Krzysztof ;
Tavener, Stewart J. ;
Wilson, Ashley J. .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2006, 45 (23) :3782-3786
[5]   Solid acids for green chemistry [J].
Clark, JH .
ACCOUNTS OF CHEMICAL RESEARCH, 2002, 35 (09) :791-797
[6]  
DONG JS, 1993, CARBON, V31, P427
[7]  
Harmer MA, 1998, ADV MATER, V10, P1255, DOI 10.1002/(SICI)1521-4095(199810)10:15<1255::AID-ADMA1255>3.0.CO
[8]  
2-T
[9]   Synthesis of new, nanoporous carbon with hexagonally ordered mesostructure [J].
Jun, S ;
Joo, SH ;
Ryoo, R ;
Kruk, M ;
Jaroniec, M ;
Liu, Z ;
Ohsuna, T ;
Terasaki, O .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2000, 122 (43) :10712-10713
[10]   Solubility of solid polycyclic aromatic hydrocarbons in pressurized hot water:: Correlation with pure component properties [J].
Karasek, Pavel ;
Planeta, Josef ;
Roth, Michal .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2006, 45 (12) :4454-4460