Conversion of colloidal ZnO-WO3 heteroaggregates into strongly blue luminescing ZnWO4 xerogels and films

被引:107
作者
Bonanni, M
Spanhel, L
Lerch, M
Fuglein, E
Muller, G
Jermann, F
机构
[1] Univ Wurzburg, Lehrstuhl Silicatchem, D-97070 Wurzburg, Germany
[2] Siemens AG, Corp Technol, D-81730 Munich, Germany
关键词
D O I
10.1021/cm9704591
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The colloidal synthesis of ZnO-WO3 heteroaggregates composed of 3-5 nm particles is presented. These sols can be used to prepare nanocrystalline ZnWO4 xerogels, powders, and thin films with strong blue fluorescence (quantum yield between 25 and 50% at room temperature). The conversion of the precursor aggregates into nano-and microcrystalline monoclinic ZnWO4 Sanmartinite has been followed by XRD, DTA-TG-MS, SEM, FTIR, optical absorption, and fluorescence methods. The ZnWO4 crystallites start to develop at 350 degrees C, and their mean crystal size increases with temperature to 35 nm at 400 degrees C and 120 nm at 600 degrees C. At the same time, the fluorescence intensity increases by 3 orders of magnitude within the aforementioned temperature regime, no matter whether X-rays or UV photons are used to excite the samples. In complementary time-resolved X-ray fluorescence investigations, two recombination processes in the micro-and millisecond range were detected. In weakly fluorescing ZnO-WO3 aggregate samples at sizes between 10 and 30 nm, the slow millisecond process dominates the recombination of the charge carriers whereas in 50-275 nm crystals and above, the faster 2.5 mu s process dominates the decay kinetics. Accordingly, the slow afterglow process is attributed to a recombination between electrons and holes deeply trapped at the surface of the heteroaggregates. The faster 2.5 mu s recombination process takes place only in the perfectly developed Sanmartinite phase.
引用
收藏
页码:304 / 310
页数:7
相关论文
共 19 条
[1]   MECHANISTIC STUDIES OF WATER DETOXIFICATION IN ILLUMINATED TIO2 SUSPENSIONS [J].
BAHNEMANN, D ;
BOCKELMANN, D ;
GOSLICH, R .
SOLAR ENERGY MATERIALS, 1991, 24 (1-4) :564-583
[2]   PHOTOELECTROCHEMISTRY OF QUANTIZED WO3 COLLOIDS - ELECTRON STORAGE, ELECTROCHROMIC, AND PHOTOELECTROCHROMIC EFFECTS [J].
BEDJA, I ;
HOTCHANDANI, S ;
KAMAT, PV .
JOURNAL OF PHYSICAL CHEMISTRY, 1993, 97 (42) :11064-11070
[3]  
Blasse G., 1994, LUMINESCENT MAT, DOI [10.1007/978-3-642-79017-1_1, DOI 10.1007/978-3-642-79017-1_1]
[4]  
Gerischer H., 1979, Solar energy conversion. Solid-state physics aspects, P115
[5]   SCINTILLATION PROPERTIES OF ZNWO4 [J].
GRASSMANN, H ;
MOSER, HG ;
LORENZ, E .
JOURNAL OF LUMINESCENCE, 1985, 33 (01) :109-113
[6]  
GREENWOOD NN, 1990, CHEM ELEMENTE, P1557
[7]   The active intermediate states, which arise in the formation of tungstates, particularly copper tungstates, in solid states [J].
Jander, W ;
Wenzel, W .
ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE, 1941, 246 (01) :67-80
[8]  
*JCPDS, 150774 JCPDS
[9]  
*JCPDS, 361451 JCPDS
[10]  
*JCPDS, 331387 JCPDS