Microstructure and electrical properties of Ni-Zn manganite ceramics

被引:18
作者
Chanel, C [1 ]
Guillemet-Fritsch, S [1 ]
Sarrias, J [1 ]
Rousset, A [1 ]
机构
[1] Univ Toulouse 3, Lab Chim Mat Inorgan & Energet, CNRS, UMR 5085, F-31062 Toulouse, France
来源
INTERNATIONAL JOURNAL OF INORGANIC MATERIALS | 2000年 / 2卷 / 2-3期
关键词
oxides; electronic materials; X-ray diffraction; electrical properties;
D O I
10.1016/S1466-6049(00)00025-8
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
Nickel zinc manganite ceramics Mn2.34Ni0.66ZnxO4 (0 less than or equal to x less than or equal to 1.02) were investigated using structure, microstructure and electrical property interrelationships. The resistivity increased with zinc content whereas the activation energy remained constant. The drift of resistivity under thermal constraint, commonly observed in NTC thermistors was almost nil when the zinc content was sufficiently high (x greater than or equal to 0.7). Homogeneous microstructures and high densities were obtained when the ceramics were prepared from fine powders. The Ni/Zn/Mn/O system prepared by 'chimie douce' has interesting NTC properties for industrial applications. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:241 / 247
页数:7
相关论文
共 16 条
[1]   IONIC ORDERING AND INFRARED-SPECTRA OF SOME II-IV SPINELS [J].
BRABERS, VAM .
PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1972, 12 (02) :629-+
[2]  
CAFFIN JP, 1986, THESIS TOULOUSE
[3]  
Chanel C., 1997, Key Engineering Materials, V132-1361, P109
[4]  
CHANEL C, 1998, THESIS TOULOUSE
[5]  
CHANEL C, IN PRESS MAT RES B
[6]   INVESTIGATIONS ON ELECTRONICALLY CONDUCTING OXIDE SYSTEMS .21. STABLE SPINELS ZNZNIMN2-ZO4 AND COMPARISON WITH SPINELS MGZNIMN2-ZO4 [J].
FELTZ, A ;
SEIDEL, A .
ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE, 1992, 608 (02) :166-172
[7]  
Feltz A., 1992, Journal of the European Ceramic Society, V9, P187, DOI 10.1016/0955-2219(92)90004-W
[8]   Correlation between the structure, the microstructure and the electrical properties of nickel manganite negative temperature coefficient (NTC) thermistors [J].
Fritsch, S ;
Sarrias, J ;
Brieu, M ;
Couderc, JJ ;
Baudour, JL ;
Snoeck, E ;
Rousset, A .
SOLID STATE IONICS, 1998, 109 (3-4) :229-237
[9]  
FRITSCH S, 1995, THESIS TOULOUSE
[10]  
Linder F., 1993, Journal of the European Ceramic Society, V11, P269, DOI 10.1016/0955-2219(93)90097-B