Fracture in ceramic-reinforced metal matrix composites based on high-speed steel

被引:38
作者
Bolton, JD [1 ]
Gant, AJ [1 ]
机构
[1] Univ Bradford, Dept Mech & Mfg Engn, Bradford BD7 1DP, W Yorkshire, England
关键词
D O I
10.1023/A:1004303609990
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A series of metal matrix composites based upon M3/2 high-speed steel was produced by a powder metal sintering route. Hard ceramic titanium carbide or niobium carbide additions and a self-lubricant in the form of manganese sulfide, were added as a basis for achieving improved wear resistance and reduced friction. After sintering, the composites were given a full standard high-speed steel heat treatment and subjected to mechanical tests. All three particulate additions had a deleterious effect on three-point bend strength, particularly in the case of MnS addition, mainly due to the ease of initiating cracks at or near to the particulate additions. Bend strengths were further reduced by the simultaneous addition of both MnS and either TiC or NbC especially when a high volume fraction of approximately 25 vol % MnS was added. Single, low volume fraction (less than or equal to 8%) additions, of TiC, NbC, or MnS, had little effect on fracture toughness and K-IC values were comparable to those found in the baseline M3/2 steel. Slight improvements in fracture toughness shown to occur in the 7.74% NbC composites were attributed to energy dissipation caused by the effects of crack branching during crack propagation. Composites with the higher volume fraction additions of MnS and ceramic carbide gave poor fracture toughness by forming MnS/carbide clusters which provided an easy path for crack propagation. (C) 1998 Chapman & Hall.
引用
收藏
页码:939 / 953
页数:15
相关论文
共 33 条
[1]  
[Anonymous], 1976, FUNDAMENTALS FRACTUR
[2]  
[Anonymous], 1994, COMPOSITE MAT ENG SC
[3]  
[Anonymous], INTRO CERAMICS
[4]  
BEISS P, 1985, MODERN DEV POWDER ME, V17, P331
[5]  
BERRY G, 1977, MET TECHNOL, V6, P289
[6]  
Bolton J. D., 1990, Powder Metallurgy, V33, P126
[7]   Heat treatment response of sintered M3/2 high speed steel composites containing additions of manganese sulphide, niobium carbide, and titanium carbide [J].
Bolton, JD ;
Gant, AJ .
POWDER METALLURGY, 1996, 39 (01) :27-35
[8]   FRACTURE-TOUGHNESS OF SINTERED METAL-MATRIX COMPOSITES BASED UPON HIGH-SPEED STEELS ENRICHED WITH HARD CERAMIC CARBIDES [J].
BOLTON, JD ;
YOUSEFFI, M .
POWDER METALLURGY, 1993, 36 (02) :142-152
[9]   PHASE REACTIONS AND CHEMICAL-STABILITY OF CERAMIC CARBIDE AND SOLID LUBRICANT PARTICULATE ADDITIONS WITHIN SINTERED HIGH-SPEED STEEL MATRIX [J].
BOLTON, JD ;
GANT, AJ .
POWDER METALLURGY, 1993, 36 (04) :267-274
[10]  
BROOKSBANK D, 1972, J IRON STEEL I, V210, P246