Development of low-toxicity gelcasting systems

被引:307
作者
Janney, MA [1 ]
Omatete, OO [1 ]
Walls, CA [1 ]
Nunn, SD [1 ]
Ogle, RJ [1 ]
Westmoreland, G [1 ]
机构
[1] Oak Ridge Natl Lab, Div Met & Ceram, Oak Ridge, TN 37831 USA
关键词
Gelcasting systems;
D O I
10.1111/j.1151-2916.1998.tb02377.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A series of low-toxicity gelcasting systems has been developed, The reagents used in these systems have very low acute toxicity. The new systems perform at least as well as, and in some cases better than, the original acrylamide-based system, The development of these systems is described herein, including the search for new gel compositions, the study of suspensions made with the new gel precursor solutions, and pyrolysis of the dried gels and gelcast parts, Applications of the new gelcasting systems include complex silicon nitride parts, large-diameter rings, rapid prototyping by green machining, and metal-powder gel casting.
引用
收藏
页码:581 / 591
页数:11
相关论文
共 13 条
[1]   STABILITY OF AQUEOUS ALPHA-AL2O3 SUSPENSIONS WITH POLY(METHACRYLIC ACID) POLY-ELECTROLYTE [J].
CESARANO, J ;
AKSAY, IA ;
BLEIER, A .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1988, 71 (04) :250-255
[2]  
Janney M. A., 1991, US Patent, Patent No. [5,028,362, 5028362, 5 028 362]
[3]  
Janney MA, 1995, P/M IN AEROSPACE, DEFENSE AND DEMANDING APPLICATIONS - 1995, P139
[4]  
JANNEY MA, 1994, DISPERSION AGGREGATI, P201
[5]  
JANNEY MA, 1997, ADV POWDER METALL 17, V5, P227
[6]  
*NAT FIR PROT ASS, 1994, NFPA 49 HAZ CHEM DAT
[7]  
Nunn S.D., 1994, J. Ceram. Eng. Sci. Proc., V15, P493
[8]  
Nunn S.D., 1996, Ceram. Eng. Sci. Proc., V17, P209
[9]  
OMATETE OO, 1991, AM CERAM SOC BULL, V70, P1641
[10]  
Taguchi G., 1990, Introduction to quality engineering