Water leaching of SrS and precipitation of SrCO3 using carbon dioxide as the precipitating agent

被引:60
作者
Owusu, G [1 ]
Litz, JE [1 ]
机构
[1] Colorado Minerals Res Inst, Golden, CO 80403 USA
关键词
water leaching; SrS; SrCO3;
D O I
10.1016/S0304-386X(00)00091-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Strontium sulphide (SrS) was water-leached at 85 degrees C, generating a saturated solution of approximately 50 g/L Sr. About 92% of the strontium contained in the SrS was leached within 60-80 min. Almost all of the water-soluble strontium were completely leached out from the sulphide material. The strontium-saturated solution was treated with carbon dioxide to precipitate strontium carbonate (SrCO3). Precipitation efficiencies in excess of 99% were attained in both batch and continuous multi-column test programs. Hydrogen sulphide gas was generated as a byproduct in the precipitation process at a slurry pH less than or equal to 8. Particle size analyses of SrCO3 precipitates indicate that a longer retention time enhances crystal growth. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:23 / 29
页数:7
相关论文
共 6 条
[1]  
Dean J. A., 1992, LANGES HDB CHEM, P5
[2]   The leaching of SrS with water and the precipitation of SrCO3 from leach solution by different carbonating agents [J].
Erdemoglu, M ;
Canbazoglu, M .
HYDROMETALLURGY, 1998, 49 (1-2) :135-150
[3]  
HOGFELDT E, 1984, STABILITY CONSTANT A, P98
[4]   THE LEACHING OF CELESTITE IN SODIUM-CARBONATE SOLUTION [J].
IWAI, M ;
TOGURI, JM .
HYDROMETALLURGY, 1989, 22 (1-2) :87-100
[5]  
POURBAIX M, 1966, ATLAS ELECTROCHEMICA, P148
[6]  
1989, CRC HDB CHEM PHYSICS