Evaluation and identification of degradative processes in post-consumer recycled high-density polyethylene

被引:69
作者
Cruz, SA [1 ]
Zanin, M [1 ]
机构
[1] Univ Fed Sao Carlos, Dept Mat Engn, BR-13565905 Sao Carlos, SP, Brazil
关键词
The authors thank Ipiranga Petroquı´mica and Ciba Specialty Chemicals for the specimens; the Brazilian research funding institution CNPq for it financial support and Dr. Gerson Mantovani for the colaboration;
D O I
10.1016/S0141-3910(02)00379-8
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
We have studied the degradation resulting from reprocessing of post-consumer HDPE in order to verify its re-stabilization needs. Cone-plate rheometry was used to provide information about the molar mass and the molar mass distribution after reprocessing and stabilizing the material. Infrared spectroscopy (FTIR), oxidation induction time (OIT), melt flow index (MFI) and cone-plate rheometry measurements were performed. Also, atomic absorption spectrophotometry tests were carried out to verify which catalytic residue was present in the recycled HDPE so as to correlate it to the degradation processes taking place in the polymer. The results showed that in this case the post-consumer HDPE displayed cross-linking when reprocessed, indicating the need for re-stabilization. They also showed that the use of 0.2% antioxidant was efficient in blocking these processes, and that the cone-plate rheometry technique was powerful in assessing degradative processes. (C) 2003 Elsevier Science Ltd., All rights reserved.
引用
收藏
页码:31 / 37
页数:7
相关论文
共 13 条
[1]  
Allen N.S., 1983, DEGRADATION STABILIZ
[2]  
Allen NS., 1992, FUNDAMENTALS POLYM D
[3]  
[Anonymous], 1992, PLASTICS RECYCLING P
[4]  
Bretas RES, 2000, REOLOGIA POLIMEROS F
[5]   Effect of catalyst residues on the chain structure and properties of a Phillips type polyethylene [J].
Epacher, E ;
Kröhnke, C ;
Pukánszky, B .
POLYMER ENGINEERING AND SCIENCE, 2000, 40 (06) :1458-1468
[6]   Recycling of post-used PE packaging film using the restabilization technique [J].
Kartalis, CN ;
Papaspyrides, CD ;
Pfaendner, R .
POLYMER DEGRADATION AND STABILITY, 2000, 70 (02) :189-197
[7]  
Kelen T., 1983, Polymer Degradation
[8]   INFLUENCE OF LOW EXTENTS OF DEGRADATION ON THE PROCESSING BEHAVIOR OF HIGH-DENSITY POLYETHYLENE [J].
LAMANTIA, FP ;
CITTA, V ;
VALENZA, A ;
ROCCASALVO, S .
POLYMER DEGRADATION AND STABILITY, 1989, 23 (02) :109-119
[9]  
MANCINI SD, 2000, PLASTICO IND, V25, P118
[10]  
Manrich S., 1999, Patent UM, Patent No. 7901580