Synthesis of biodegradable poly(ester amide)s containing functional groups

被引:13
作者
Guan, HL [1 ]
Deng, C [1 ]
Xu, XY [1 ]
Liang, QZ [1 ]
Chen, XS [1 ]
Jing, XB [1 ]
机构
[1] Chinese Acad Sci, Changchun Inst Appl Chem, State Key Lab Polymer Phys & Chem, Changchun 130022, Peoples R China
关键词
biopolymers; functionalization of polymers; interfacial polycondensation; modification of polyesters; poly(ester amide)s;
D O I
10.1002/pola.20590
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 [高分子化学与物理]; 080501 [材料物理与化学]; 081704 [应用化学];
摘要
A series of aliphatic poly(ester amide)s containing functional groups were prepared using a two-step polycondensation. The composition and properties of the poly(ester amide)s were characterized with dimethylolpropionic acid (DMPA), a diamine derived from glycine and sebacoyl dichloride. It was observed that the diol monomer DMPA entered the chain of the synthesized poly(ester amide)s, and the benzyl ester group could be removed by catalytic hydrogenolysis. The melting temperature and Tg of the poly(ester amide)s was found to be approximately 150 and 0 °C.
引用
收藏
页码:1144 / 1149
页数:6
相关论文
共 36 条
[1]
Armelin E, 2002, MACROMOL CHEM PHYSIC, V203, P48, DOI 10.1002/1521-3935(20020101)203:1<48::AID-MACP48>3.0.CO
[2]
2-E
[3]
Study on the degradability of poly(ester amide)s derived from the α-amino acids glycine, and L-alanine containing a variable amide/ester ratio [J].
Armelin, E ;
Paracuellos, N ;
Rodríguez-Galán, A ;
Puiggalí, J .
POLYMER, 2001, 42 (19) :7923-7932
[4]
COMPOSITES OF NOVEL BIODEGRADABLE COPOLYAMIDES BASED ON ADIPIC ACID, 1,6-HEXANE DIAMINE AND L-PROLINE WITH SHORT E-GLASS FIBERS .1. PREPARATION AND PROPERTIES [J].
ARVANITOYANNIS, I ;
PSOMIADOU, E ;
YAMAMOTO, N ;
BLANSHARD, JMV .
POLYMER, 1995, 36 (03) :493-503
[5]
SYNTHESIS AND PHYSICO-MECHANICAL PROPERTIES OF ALIPHATIC POLYESTERAMIDES [J].
CASTALDO, L ;
DECANDIA, F ;
MAGLIO, G ;
PALUMBO, R ;
STRAZZA, G .
JOURNAL OF APPLIED POLYMER SCIENCE, 1982, 27 (05) :1809-1822
[6]
SEGMENTED COPOLYMERS WITH POLY(ESTER AMIDE) UNITS OF UNIFORM LENGTH - SYNTHESIS [J].
GAYMANS, RJ ;
DEHAAN, JL .
POLYMER, 1993, 34 (20) :4360-4364
[7]
DEGRADATION OF NONALTERNATING POLY(ESTER-AMIDES) [J].
GONSALVES, KE ;
CHEN, X ;
CAMERON, JA .
MACROMOLECULES, 1992, 25 (12) :3309-3312
[8]
Hile DD, 2001, J POLYM SCI POL CHEM, V39, P562, DOI 10.1002/1099-0518(20010215)39:4<562::AID-POLA1027>3.0.CO
[9]
2-L
[10]
HOLLAND S J, 1986, Journal of Controlled Release, V4, P155, DOI 10.1016/0168-3659(86)90001-5