New manganese dioxides for lithium batteries

被引:24
作者
Bowden, W. [1 ]
Bofinger, T.
Zhang, F.
Iltchev, N.
Sirotina, R.
Paik, Y.
Chen, H.
Grey, C.
Hackney, S.
机构
[1] Gillette Technol Ctr US, Needham, MA 02492 USA
[2] SUNY Stony Brook, Stony Brook, NY 11794 USA
[3] Michigan Technol Univ, Houghton, MI 49931 USA
关键词
manganese dioxide; lithium battery; ion exchange; cation vacancy; SPECS; MAS NMR;
D O I
10.1016/j.jpowsour.2006.10.041
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Lithium/manganese dioxide primary batteries use heat treated manganese dioxide (HEMD), a defect pyrolusite structure material as the cathode active material. Ion exchange of the structural protons in electrolytic manganese dioxide (EMD) with lithium before heating results in formation of a lithium containing gamma-MnO2. Increased lithium hydroxide concentration and increased temperature lead to increased lithium levels. At 80 degrees C with a combination of LiOH and LiBr, almost all of the structural protons in MnO2 are replaced by lithium resulting in a gamma-MnO2 phase substantially free of protons and containing about 1.8% Li. This highly substituted lithium containing MnO2 is reduced at between 3.5 and 1.8 V and has a capacity of 250 mAh g(-1). There are two reduction processes, one at 3.25 and the other at 2.9 V. TGA studies reveal two processes during heat treatment. Heating the lithium substituted MnO2 to 350-400 degrees C results in a partially ordered HEMD-like MnO2 (LiMD) phase with higher running voltage and superior discharge kinetics. Continued heating of the lithiated manganese dioxide to 450-480 degrees C under oxygen partial pressure can result in formation of a mixed phase containing both HEMD and a new, ordered MnO2 phase (OMD). The intimately mixed HEMD/OMD composition has a discharge voltage near 2.9 V with a capacity about 220 mAh g(-1). Heating exhaustively lithiated MnO2 to 350-400 degrees C results in formation of the partially ordered LiMD MnO2 phase as with the previous partially lithium substituted MnO2. Additional heating of the highly lithium substituted MnO2 to 450-480 degrees C under oxygen results in formation of the new OMD phase in substantially pure form. Discharge of the new OMD phase shows it has a discharge capacity near 200 mAh g(-1) between 3.4 and 2.4 V versus lithium in a single, well-defined discharge process. OMD demonstrated good cycling against Li with no indication of formation of LiMn2O4 spinel after 80 deep discharge cycles. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:609 / 615
页数:7
相关论文
共 18 条
[1]   Lithiation of ramsdellite-pyrolusite MnO2;: NMR, XRD, TEM and electrochemical investigation of the discharge mechanism [J].
Bowden, W ;
Grey, CP ;
Hackney, S ;
Wang, F ;
Paik, Y ;
Iltchev, N ;
Sirotina, R .
JOURNAL OF POWER SOURCES, 2006, 153 (02) :265-273
[2]  
BOWDEN W, 1997, Patent No. 5698176
[3]  
BOWDEN W, 2002, ITE LETT, V3, pB1
[4]  
BOWDEN W, 2000, ITE LETT, V1, pB27
[5]  
CAPPARELLA M, 1999, Patent No. 5863675
[6]   STRUCTURAL AND ELECTROCHEMICAL PROPERTIES OF THE PROTON GAMMA-MNO2 SYSTEM [J].
CHABRE, Y ;
PANNETIER, J .
PROGRESS IN SOLID STATE CHEMISTRY, 1995, 23 (01) :1-130
[7]  
Christian P. A., 2002, U.S. Patent, Patent No. [6,403,257, 6403257]
[8]   On the structural defects in synthetic γ-MnO2S [J].
Hill, LI ;
Verbaere, A .
JOURNAL OF SOLID STATE CHEMISTRY, 2004, 177 (12) :4706-4723
[9]  
IKEDA, 1975, P MANG DIOX S CLEV, V1
[10]  
ILTCHEV N, 2001, Patent No. 6190800