Promoted Fe/ZSM-5 catalysts prepared by sublimation:: de-NOx activity and durability in H2O-rich streams

被引:139
作者
Chen, HY [1 ]
Sachtler, WMH [1 ]
机构
[1] Northwestern Univ, Ctr Catalysis & Surface Sci, VN Ipatieff Lab, Dept Chem, Evanston, IL 60208 USA
关键词
de-NOx in lean burn emissions; SCR of NOx; promoted Fe/ZSM-5; catalyst durability;
D O I
10.1023/A:1019079305250
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Fe/ZSM-5 catalysts with an Fe/Al ratio approximate to 1.0, were prepared by sublimation of FeCl3 into H/ZSM-5. They display high activity and durability for the selective catalytic reduction of NOx to N-2, both in dry and wet gas flows. These catalysts have now been modified by exchanging a second cation into the zeolite. Mere neutralization of zeolite protons by Naf lowers the selectivity for NOx reduction to N-2, but the cations Ce3+ and La3+ act as true catalyst promoters. With isobutane as the reductant in a simulated vehicular emission gas, almost 90% of NOx is reduced to N-2 at 350 degrees C over the La-promoted catalyst. The presence of 10% H2O in the feed does not impair the catalyst performance at high temperature; in the temperature region below 350 degrees C it even increases the N-2 yield. The beneficial effect of La is due to its lowering of the catalyst activity for the undesired combustion of the hydrocarbon. No signs of zeolite destruction are evident after 100 h TOS in a wet gas flow at 350 degrees C. Carbonaceous deposits causing a slight deactivation are easily removed in an O-2/He flow at 500 degrees C; this in situ regeneration fully restores the original activity.
引用
收藏
页码:125 / 130
页数:6
相关论文
共 15 条
  • [1] The effect of zeolitic protons on NOx reduction over Pd/ZSM-5 catalysts
    Adelman, BJ
    Sachtler, WMH
    [J]. APPLIED CATALYSIS B-ENVIRONMENTAL, 1997, 14 (1-2) : 1 - 11
  • [2] Mechanistic cause of hydrocarbon specificity over Cu/ZSM-5 and Co/ZSM-5 catalysts in the selective catalytic reduction of NOx
    Adelman, BJ
    Beutel, T
    Lei, GD
    Sachtler, WMH
    [J]. JOURNAL OF CATALYSIS, 1996, 158 (01) : 327 - 335
  • [3] CHEN HY, IN PRESS CATAL TODAY
  • [4] COTTON FA, 1988, ADV INORG CHEM, P717
  • [5] Limitations on the formation of oxygen-bridged divalent cations in FeZSM-5
    Feng, XB
    Hall, WK
    [J]. CATALYSIS LETTERS, 1997, 46 (1-2) : 11 - 16
  • [6] FeZSM-5: A durable SCR catalyst for NOx removal from combustion streams
    Feng, XB
    Hall, WK
    [J]. JOURNAL OF CATALYSIS, 1997, 166 (02) : 368 - 376
  • [7] On the unusual stability of overexchanged FeZSM-5
    Feng, XB
    Hall, WK
    [J]. CATALYSIS LETTERS, 1996, 41 (1-2) : 45 - 46
  • [8] Unusual structure and stability of iron-oxygen nano-clusters in Fe-ZSM-5 catalysts
    Joyner, RW
    Stockenhuber, M
    [J]. CATALYSIS LETTERS, 1997, 45 (1-2) : 15 - 19
  • [9] Lunin VV, 1996, DOKL AKAD NAUK+, V349, P638
  • [10] CHARACTERIZATION OF IRON SPECIES IN Y-TYPE ZEOLITE AND MODIFIED FORM OF THE ZEOLITE
    MAEDA, Y
    KATO, N
    KAWASAKI, S
    TAKASHIMA, Y
    HIDAKA, S
    NITA, K
    [J]. ZEOLITES, 1990, 10 (01): : 21 - 27