共 30 条
[1]
QUASI-STATIC CONSTITUTIVE BEHAVIOR OF ZR41.25TI13.75NI10CU12.5BE22.5 BULK AMORPHOUS-ALLOYS
[J].
SCRIPTA METALLURGICA ET MATERIALIA,
1994, 30 (04)
:429-434
[3]
COMPRESSIVE DEFORMATION OF AMORPHOUS PD40NI40P20
[J].
MATERIALS SCIENCE AND ENGINEERING,
1988, 98
:487-490
[6]
Fischer-Cripps A.C., 2002, MECH ENG S
[7]
FLOES KM, 2002, J MATER RES, V17, P1153
[8]
Mechanisms for fracture and fatigue-crack propagation in a bulk metallic glass
[J].
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1999, 30 (07)
:1739-1753
[9]
PRODUCTION OF AMORPHOUS CO-SI-B AND CO-M-SI-B (M = GROUP-IV - VIII TRANSITION-METALS) WIRES BY A METHOD EMPLOYING MELT SPINNING INTO ROTATING WATER AND SOME PROPERTIES OF THE WIRES
[J].
MATERIALS SCIENCE AND ENGINEERING,
1982, 54 (02)
:197-207