Mechanical property and dimensional stability of substrates for magnetic tapes

被引:27
作者
Higashioji, T [1 ]
Tsunekawa, T
Bhushan, B
机构
[1] Toray Industries Ltd, Films & Film Prod Res Labs, Otsu, Shiga, Japan
[2] Ohio State Univ, Dept Mech Engn, Nanotribol Lab Informat Storage & MEMS NEMS, Columbus, OH 43210 USA
关键词
mechanical property; dimensional stability; magnetic tape;
D O I
10.1016/S0301-679X(02)00232-3
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We have performed a comparative study on mechanical property and dimensional stability of substrates for magnetic tapes. The substrates include polyethylene terephthalate (PET), polyethylene naphthalate (PEN), and aromatic polyamide (ARAMID), which could be used for linear-type magnetic tapes for computer data storage. We have demonstrated that ARAMID is the most attractive substrate and that PET has the advantage of considerably smaller irreversible creep deformation and lateral contraction caused by tension as compared to PEN film. In this paper, we also introduce recently developed PET (Advanced PET) with higher glass transition temperature compared to conventional PET; moreover, we discuss the relationship between film properties and polymeric structures of these substrates. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:437 / 445
页数:9
相关论文
共 18 条
[1]   Influence of liquid crystalline order on the dielectric relaxation of random copolyesters of PET, PEN, and PHB [J].
Ahumada, O ;
Ezquerra, TA ;
Nogales, A ;
BaltaCalleja, FJ ;
Zachmann, HG .
MACROMOLECULES, 1996, 29 (14) :5002-5009
[2]  
[Anonymous], 1983, INTRO POLYM VISCOELA
[3]   THERMAL SHRINKAGE OF ORIENTED SEMICRYSTALLINE POLY(ETHYLENE TEREPHTHALATE) [J].
BHATT, GM ;
BELL, JP .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1976, 14 (04) :575-590
[4]  
Bhushan B, 2002, J APPL POLYM SCI, V83, P2225, DOI 10.1002/app10194
[5]  
Bhushan B., 2000, MECH RELIABILITY FLE, DOI [10.1007/978-1-4612-1266-9, DOI 10.1007/978-1-4612-1266-9]
[6]  
Bhushan B., 1996, TRIBOLOGY MECH MAGNE, DOI 10.1007/978-1-4612-2364-1
[7]   THE B-LOSS PROCESS IN LIQUID-CRYSTAL POLYESTERS CONTAINING 2,6-NAPHTHYL GROUPS [J].
BLUNDELL, DJ ;
BUCKINGHAM, KA .
POLYMER, 1985, 26 (11) :1623-1627
[8]   GLASS-TRANSITION TEMPERATURE OF COPOLYESTERS OF PET, PEN AND PHB AS DETERMINED BY DYNAMIC MECHANICAL ANALYSIS [J].
CHEN, D ;
ZACHMANN, HG .
POLYMER, 1991, 32 (09) :1612-1621
[9]   DIELECTRIC-RELAXATION OF AMORPHOUS RANDOM COPOLYMERS OF POLY(ETHYLENE-TEREPHTHALATE) AND POLY(ETHYLENE-2,6-NAPHTHALENE DICARBOXYLATE) [J].
EZQUERRA, TA ;
BALTACALLEJA, FJ ;
ZACHMANN, HG .
ACTA POLYMERICA, 1993, 44 (01) :18-24
[10]  
GILLMOR JR, 1997, P SOC PLASTIC ENG AN, V97, P1582