Stress corrosion crack propagation in AerMet 100

被引:49
作者
Oehlert, A [1 ]
Atrens, A [1 ]
机构
[1] Univ Queensland, Dept Min Minerals & Mat Engn, Brisbane, Qld 4072, Australia
关键词
D O I
10.1023/A:1004362400904
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture mechanics tests were carried out for AerMet 100 in distilled water and NaCl (3.5 and 35 gl(-1)). The initiation period at higher values of the stress intensity factor indicated that load application in the stress corrosion cracking (SCC) environment is a necessary but not sufficient factor for SCC and that time is needed for some other factor (e.g., the local hydrogen concentration) to reach an appropriate value. The threshold stress intensity factor, K-ISSC, was found to increase with decreasing NaCl concentration. The plateau stress corrosion crack velocity was 2 x 10(-8) ms(-1) for NaCl (3.5 and 35 gl(-1)). The fracture mode was transgranular with small areas of an intergranular nature. (C) 1998 Chapman & Hall.
引用
收藏
页码:775 / 781
页数:7
相关论文
共 28 条
[1]   LINEARLY INCREASING STRESS TEST (LIST) FOR SCC RESEARCH [J].
ATRENS, A ;
BROSNAN, CC ;
RAMAMURTHY, S ;
OEHLERT, A ;
SMITH, IO .
MEASUREMENT SCIENCE AND TECHNOLOGY, 1993, 4 (11) :1281-1292
[2]  
Atrens A, 1995, MATER FORUM, V19, P9
[3]  
Atrens A., 1989, Advances in Fracture Research. Proceedings of the 7th International Conference on Fracture (ICF7), P1603
[4]  
ATRENS A, 1993, MATER FORUM, V17, P263
[5]  
EHLERS R, 1984, MAT TECH, V4, P127
[6]  
GATES JD, 1987, Z WERKSTOFFTECH, V18, P344, DOI 10.1002/mawe.19870181011
[7]  
GATES JD, 1987, Z WERKSTOFFTECH, V18, P179, DOI 10.1002/mawe.19870180607
[8]  
GATES JD, 1987, Z WERKSTOFFTECH, V18, P165, DOI 10.1002/mawe.19870180508
[9]  
HEMPHILL RM, 1992, Patent No. 5087415
[10]   ESCA-STUDIES OF THE STRUCTURE AND COMPOSITION OF THE PASSIVE FILM FORMED ON STAINLESS-STEELS BY VARIOUS IMMERSION TIMES IN 0.1 M NACL SOLUTION [J].
JIN, S ;
ATRENS, A .
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 1987, 42 (02) :149-165