The true fundamental trends of the different phase transformation steps (Fe2O3-Fe3O4-FeO-Fe) during iron oxide reduction process are necessary requested. Both of the macroscopic and microscopic changes during these steps have a direct bearing on the overall reduction kinetics. Magnetite single crystals were isothermally reduced in pure hydrogen at 900-1100 degrees C. The oxygen weight loss during reduction process was recorded as a function of time. The magnetite samples and its reduction products were characterized by X-ray diffraction analysis, reflected light microscope, scanning electron microscope and vibrating sample magnetometer to reveal the effect of hydrogen reduction at different temperatures on reduction behavior, composition, microstructure and magnetic properties of the produced samples. The reduction rate increases with reaction temperature. The reduction at 900 and 950 degrees C was stopped at 83 and 89% extent, respectively. Depending on the kinetics obtained data from reduction process, the reduction rate was found to be controlled by the solid-state diffusion mechanism. The magnetic characterizations of the reduced magnetite at 900-1100 degrees C were measured whereas the magnetization value increased from 114.1 to 132.1 emu/g with increasing temperature. Magnetite single crystal was partially reduced at 20,40, 60, and 80%, its magnetic properties was found to be dependent on the morphology, core-shell like structure is formed at 40% reduction extent. (C) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:251 / 258
页数:8
相关论文
共 16 条
[1]  
BAHGAT M, 2005, ISIJ INT, V45
[2]  
BRAHMA D, 1988, STEEL RES, V59, P532
[3]   EFFECT OF HYDROGEN REDUCTION TEMPERATURE ON THE SURFACE-CHEMISTRY OF PURE AND PROMOTED MAGNETITE [J].
CACERES, PG .
APPLIED CATALYSIS A-GENERAL, 1994, 110 (02) :185-196
[4]   MICROSTRUCTURAL AND SURFACE-AREA DEVELOPMENT DURING HYDROGEN REDUCTION OF MAGNETITE [J].
CACERES, PG ;
BEHBEHANI, MH .
APPLIED CATALYSIS A-GENERAL, 1994, 109 (02) :211-223
[5]  
CHEN Q, 1998, J CENT SOUTH UNIV T, V5, P1
[6]   Behaviour of manganese oxides during magnetising reduction of Baharia iron ore by CO-CO2 gas mixture [J].
El-Geassy, AA ;
Nasr, MI ;
Yousef, MA ;
Khedr, MH ;
Bahgat, M .
IRONMAKING & STEELMAKING, 2000, 27 (02) :117-122
[7]  
El-Geassy AHA, 1998, SCAND J METALL, V27, P205
[8]  
Hafeli U., 1997, Scientific and Clinical Applications of Magnetic Carriers, DOI DOI 10.1007/s10439-009-9660-y
[9]  
HAYES PC, 1990, METALL T B, V21, P743
[10]   Isothermal reduction kinetics of Fe2O3 mixed with 1-10% Cr2O3 at 1173-1473 K [J].
Khedr, MH .
ISIJ INTERNATIONAL, 2000, 40 (04) :309-314